General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación transversal | 20.0 °C | 18 % Show Material materials with Elongación transversal of 18 % | |
Límite elástico | 20.0 °C | 415 MPa Show Material materials with Límite elástico of 415 MPa | |
Límite elástico transversal | 20.0 °C | 415 MPa Show Material materials with Límite elástico transversal of 415 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 550 - 700 MPa Show Material materials with Resistencia a la tracción of 550 - 700 MPa | |
Resistencia a la tracción transversal | 20.0 °C | 550 - 700 MPa Show Material materials with Resistencia a la tracción transversal of 550 - 700 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.14 % Show Material materials with Carbono of 0.14 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 - 1.6 % Show Material materials with Manganeso of 1 - 1.6 % |
Silicona | 0.45 % Show Material materials with Silicona of 0.45 % |