General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.84 g/cm³ Show Material materials with Densidad of 7.84 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Dureza Brinell | 20.0 °C | 205 - 250 [-] Show Material materials with Dureza Brinell of 205 - 250 [-] | |
Elongación | 20.0 °C | 16 % Show Material materials with Elongación of 16 % | |
Estricción | 20.0 °C | 60 % Show Material materials with Estricción of 60 % | |
Límite elástico Rp 0,2 | 20.0 °C | 550 MPa Show Material materials with Límite elástico Rp 0,2 of 550 MPa | |
200.0 °C | 500 MPa Show Material materials with Límite elástico Rp 0,2 of 500 MPa | ||
250.0 °C | 480 MPa Show Material materials with Límite elástico Rp 0,2 of 480 MPa | ||
300.0 °C | 460 MPa Show Material materials with Límite elástico Rp 0,2 of 460 MPa | ||
350.0 °C | 441 MPa Show Material materials with Límite elástico Rp 0,2 of 441 MPa | ||
400.0 °C | 412 MPa Show Material materials with Límite elástico Rp 0,2 of 412 MPa | ||
450.0 °C | 372 MPa Show Material materials with Límite elástico Rp 0,2 of 372 MPa | ||
500.0 °C | 334 MPa Show Material materials with Límite elástico Rp 0,2 of 334 MPa | ||
550.0 °C | 275 MPa Show Material materials with Límite elástico Rp 0,2 of 275 MPa | ||
Módulo elástico | -100.0 °C | 217 GPa Show Material materials with Módulo elástico of 217 GPa | |
20.0 °C | 212 GPa Show Material materials with Módulo elástico of 212 GPa | ||
100.0 °C | 204 - 207 GPa Show Material materials with Módulo elástico of 204 - 207 GPa | ||
200.0 °C | 196 - 199 GPa Show Material materials with Módulo elástico of 196 - 199 GPa | ||
300.0 °C | 186 - 192 GPa Show Material materials with Módulo elástico of 186 - 192 GPa | ||
400.0 °C | 177 - 184 GPa Show Material materials with Módulo elástico of 177 - 184 GPa | ||
500.0 °C | 164 - 175 GPa Show Material materials with Módulo elástico of 164 - 175 GPa | ||
600.0 °C | 127 - 164 GPa Show Material materials with Módulo elástico of 127 - 164 GPa | ||
Resistencia a la tracción | 20.0 °C | 700 - 850 MPa Show Material materials with Resistencia a la tracción of 700 - 850 MPa | |
300.0 °C | 590 MPa Show Material materials with Resistencia a la tracción of 590 MPa | ||
350.0 °C | 560 MPa Show Material materials with Resistencia a la tracción of 560 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | -100.0 °C | 423 J/(kg·K) Show Material materials with Calor específico of 423 J/(kg·K) | |
20.0 °C | 461 J/(kg·K) Show Material materials with Calor específico of 461 J/(kg·K) | ||
100.0 °C | 479 J/(kg·K) Show Material materials with Calor específico of 479 J/(kg·K) | ||
200.0 °C | 499 J/(kg·K) Show Material materials with Calor específico of 499 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) Show Material materials with Calor específico of 517 J/(kg·K) | ||
400.0 °C | 536 J/(kg·K) Show Material materials with Calor específico of 536 J/(kg·K) | ||
500.0 °C | 558 J/(kg·K) Show Material materials with Calor específico of 558 J/(kg·K) | ||
600.0 °C | 587 J/(kg·K) Show Material materials with Calor específico of 587 J/(kg·K) | ||
Coeficiente de dilatación térmica | -100.0 °C | 1.05E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.05E-5 1/K | |
20.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | ||
100.0 °C | 1.11E-5 - 1.21E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.11E-5 - 1.21E-5 1/K | ||
200.0 °C | 1.21E-5 - 1.27E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.21E-5 - 1.27E-5 1/K | ||
300.0 °C | 1.29E-5 - 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29E-5 - 1.32E-5 1/K | ||
400.0 °C | 1.35E-5 - 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 - 1.36E-5 1/K | ||
500.0 °C | 1.39E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.39E-5 - 1.4E-5 1/K | ||
600.0 °C | 1.41E-5 - 1.44E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.41E-5 - 1.44E-5 1/K | ||
Conductividad térmica | 20.0 °C | 34.6 W/(m·K) Show Material materials with Conductividad térmica of 34.6 W/(m·K) | |
100.0 °C | 36.9 W/(m·K) Show Material materials with Conductividad térmica of 36.9 W/(m·K) | ||
200.0 °C | 37.3 W/(m·K) Show Material materials with Conductividad térmica of 37.3 W/(m·K) | ||
300.0 °C | 36.9 W/(m·K) Show Material materials with Conductividad térmica of 36.9 W/(m·K) | ||
400.0 °C | 35.8 W/(m·K) Show Material materials with Conductividad térmica of 35.8 W/(m·K) | ||
500.0 °C | 34.4 W/(m·K) Show Material materials with Conductividad térmica of 34.4 W/(m·K) | ||
600.0 °C | 32.9 W/(m·K) Show Material materials with Conductividad térmica of 32.9 W/(m·K) | ||
Difusividad térmica | 20.0 °C | 9.6 mm²/s Show Material materials with Difusividad térmica of 9.6 mm²/s | |
100.0 °C | 9.5 mm²/s Show Material materials with Difusividad térmica of 9.5 mm²/s | ||
200.0 °C | 9 mm²/s Show Material materials with Difusividad térmica of 9 mm²/s | ||
300.0 °C | 8.4 mm²/s Show Material materials with Difusividad térmica of 8.4 mm²/s | ||
400.0 °C | 7.6 mm²/s Show Material materials with Difusividad térmica of 7.6 mm²/s | ||
500.0 °C | 6.6 mm²/s Show Material materials with Difusividad térmica of 6.6 mm²/s | ||
600.0 °C | 5.5 mm²/s Show Material materials with Difusividad térmica of 5.5 mm²/s | ||
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Temperatura máx. de funcionamiento, largo | 0 - 540 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 540 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 3.01E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.01E-7 Ω·m |
100.0 °C | 3.47E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.47E-7 Ω·m | |
200.0 °C | 4.23E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.23E-7 Ω·m | |
300.0 °C | 5.09E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.09E-7 Ω·m | |
400.0 °C | 6.08E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.08E-7 Ω·m | |
500.0 °C | 7.19E-7 Ω·m Show Material materials with Resistividad eléctrica of 7.19E-7 Ω·m | |
600.0 °C | 8.43E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.43E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.17 - 0.25 % Show Material materials with Carbono of 0.17 - 0.25 % |
Cromo | 1.2 - 1.5 % Show Material materials with Cromo of 1.2 - 1.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.35 - 0.85 % Show Material materials with Manganeso of 0.35 - 0.85 % |
Molibdeno | 0.65 - 0.8 % Show Material materials with Molibdeno of 0.65 - 0.8 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |
Vanadio | 0.25 - 0.35 % Show Material materials with Vanadio of 0.25 - 0.35 % |