General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.83 g/cm³ Show Material materials with Densidad of 7.83 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.28 [-] Show Material materials with Coeficiente de Poisson of 0.28 [-] |
Dureza Brinell | 20.0 °C | 250 - 295 [-] Show Material materials with Dureza Brinell of 250 - 295 [-] |
Elongación | 20.0 °C | 14 % Show Material materials with Elongación of 14 % |
Estricción | 20.0 °C | 45 % Show Material materials with Estricción of 45 % |
Límite elástico Rp 0,2 | 20.0 °C | 700 MPa Show Material materials with Límite elástico Rp 0,2 of 700 MPa |
200.0 °C | 635 MPa Show Material materials with Límite elástico Rp 0,2 of 635 MPa | |
250.0 °C | 617 MPa Show Material materials with Límite elástico Rp 0,2 of 617 MPa | |
300.0 °C | 598 MPa Show Material materials with Límite elástico Rp 0,2 of 598 MPa | |
350.0 °C | 578 MPa Show Material materials with Límite elástico Rp 0,2 of 578 MPa | |
400.0 °C | 540 MPa Show Material materials with Límite elástico Rp 0,2 of 540 MPa | |
450.0 °C | 500 MPa Show Material materials with Límite elástico Rp 0,2 of 500 MPa | |
500.0 °C | 460 MPa Show Material materials with Límite elástico Rp 0,2 of 460 MPa | |
550.0 °C | 403 MPa Show Material materials with Límite elástico Rp 0,2 of 403 MPa | |
Módulo elástico | -100.0 °C | 217 GPa Show Material materials with Módulo elástico of 217 GPa |
20.0 °C | 212 GPa Show Material materials with Módulo elástico of 212 GPa | |
100.0 °C | 204 - 207 GPa Show Material materials with Módulo elástico of 204 - 207 GPa | |
200.0 °C | 196 - 199 GPa Show Material materials with Módulo elástico of 196 - 199 GPa | |
300.0 °C | 186 - 192 GPa Show Material materials with Módulo elástico of 186 - 192 GPa | |
400.0 °C | 177 - 184 GPa Show Material materials with Módulo elástico of 177 - 184 GPa | |
500.0 °C | 164 - 175 GPa Show Material materials with Módulo elástico of 164 - 175 GPa | |
600.0 °C | 127 - 164 GPa Show Material materials with Módulo elástico of 127 - 164 GPa | |
Resistencia a la tracción | 20.0 °C | 850 - 1000 MPa Show Material materials with Resistencia a la tracción of 850 - 1000 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | -100.0 °C | 423 J/(kg·K) Show Material materials with Calor específico of 423 J/(kg·K) | |
20.0 °C | 461 J/(kg·K) Show Material materials with Calor específico of 461 J/(kg·K) | ||
100.0 °C | 479 J/(kg·K) Show Material materials with Calor específico of 479 J/(kg·K) | ||
200.0 °C | 499 J/(kg·K) Show Material materials with Calor específico of 499 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) Show Material materials with Calor específico of 517 J/(kg·K) | ||
400.0 °C | 536 J/(kg·K) Show Material materials with Calor específico of 536 J/(kg·K) | ||
500.0 °C | 558 J/(kg·K) Show Material materials with Calor específico of 558 J/(kg·K) | ||
600.0 °C | 587 J/(kg·K) Show Material materials with Calor específico of 587 J/(kg·K) | ||
Coeficiente de dilatación térmica | -100.0 °C | 1.05E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.05E-5 1/K | |
20.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | ||
100.0 °C | 1.11E-5 - 1.21E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.11E-5 - 1.21E-5 1/K | ||
200.0 °C | 1.21E-5 - 1.27E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.21E-5 - 1.27E-5 1/K | ||
300.0 °C | 1.29E-5 - 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29E-5 - 1.32E-5 1/K | ||
400.0 °C | 1.35E-5 - 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 - 1.36E-5 1/K | ||
500.0 °C | 1.39E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.39E-5 - 1.4E-5 1/K | ||
600.0 °C | 1.41E-5 - 1.44E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.41E-5 - 1.44E-5 1/K | ||
Conductividad térmica | 20.0 °C | 45.1 W/(m·K) Show Material materials with Conductividad térmica of 45.1 W/(m·K) | |
100.0 °C | 45.1 W/(m·K) Show Material materials with Conductividad térmica of 45.1 W/(m·K) | ||
200.0 °C | 44.1 W/(m·K) Show Material materials with Conductividad térmica of 44.1 W/(m·K) | ||
300.0 °C | 41.9 W/(m·K) Show Material materials with Conductividad térmica of 41.9 W/(m·K) | ||
400.0 °C | 39.4 W/(m·K) Show Material materials with Conductividad térmica of 39.4 W/(m·K) | ||
500.0 °C | 36.9 W/(m·K) Show Material materials with Conductividad térmica of 36.9 W/(m·K) | ||
600.0 °C | 34.4 W/(m·K) Show Material materials with Conductividad térmica of 34.4 W/(m·K) | ||
Difusividad térmica | 20.0 °C | 12.5 mm²/s Show Material materials with Difusividad térmica of 12.5 mm²/s | |
100.0 °C | 11.6 mm²/s Show Material materials with Difusividad térmica of 11.6 mm²/s | ||
200.0 °C | 10.6 mm²/s Show Material materials with Difusividad térmica of 10.6 mm²/s | ||
300.0 °C | 9.5 mm²/s Show Material materials with Difusividad térmica of 9.5 mm²/s | ||
400.0 °C | 8.4 mm²/s Show Material materials with Difusividad térmica of 8.4 mm²/s | ||
500.0 °C | 7.1 mm²/s Show Material materials with Difusividad térmica of 7.1 mm²/s | ||
600.0 °C | 5.8 mm²/s Show Material materials with Difusividad térmica of 5.8 mm²/s | ||
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Temperatura máx. de funcionamiento, largo | 0 - 540 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 540 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 2.31E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.31E-7 Ω·m |
100.0 °C | 2.84E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.84E-7 Ω·m | |
200.0 °C | 3.58E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.58E-7 Ω·m | |
300.0 °C | 4.48E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.48E-7 Ω·m | |
400.0 °C | 5.52E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.52E-7 Ω·m | |
500.0 °C | 6.71E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.71E-7 Ω·m | |
600.0 °C | 8.06E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.06E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.36 - 0.44 % Show Material materials with Carbono of 0.36 - 0.44 % |
Cromo | 0.9 - 1.2 % Show Material materials with Cromo of 0.9 - 1.2 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.35 - 0.85 % Show Material materials with Manganeso of 0.35 - 0.85 % |
Molibdeno | 0.6 - 0.75 % Show Material materials with Molibdeno of 0.6 - 0.75 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |
Vanadio | 0.25 - 0.35 % Show Material materials with Vanadio of 0.25 - 0.35 % |