General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.82 g/cm³ Show Material materials with Densidad of 7.82 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel |
Elongación | 20.0 °C | 20 - 22 % Show Material materials with Elongación of 20 - 22 % | |
Límite elástico Rp 0,2 | 20.0 °C | 260 MPa Show Material materials with Límite elástico Rp 0,2 of 260 MPa | |
100.0 °C | 245 MPa Show Material materials with Límite elástico Rp 0,2 of 245 MPa | ||
150.0 °C | 225 MPa Show Material materials with Límite elástico Rp 0,2 of 225 MPa | ||
200.0 °C | 210 MPa Show Material materials with Límite elástico Rp 0,2 of 210 MPa | ||
250.0 °C | 190 MPa Show Material materials with Límite elástico Rp 0,2 of 190 MPa | ||
300.0 °C | 170 MPa Show Material materials with Límite elástico Rp 0,2 of 170 MPa | ||
350.0 °C | 150 MPa Show Material materials with Límite elástico Rp 0,2 of 150 MPa | ||
400.0 °C | 130 MPa Show Material materials with Límite elástico Rp 0,2 of 130 MPa | ||
450.0 °C | 105 MPa Show Material materials with Límite elástico Rp 0,2 of 105 MPa | ||
Módulo de cizallamiento | 23.0 °C | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel |
Módulo elástico | -100.0 °C | 217 GPa Show Material materials with Módulo elástico of 217 GPa | |
20.0 °C | 212 GPa Show Material materials with Módulo elástico of 212 GPa | ||
100.0 °C | 207 GPa Show Material materials with Módulo elástico of 207 GPa | ||
200.0 °C | 199 - 200 GPa Show Material materials with Módulo elástico of 199 - 200 GPa | ||
300.0 °C | 192 - 193 GPa Show Material materials with Módulo elástico of 192 - 193 GPa | ||
400.0 °C | 184 GPa Show Material materials with Módulo elástico of 184 GPa | ||
500.0 °C | 175 GPa Show Material materials with Módulo elástico of 175 GPa | ||
600.0 °C | 164 GPa Show Material materials with Módulo elástico of 164 GPa | ||
Resistencia a la tracción | 20.0 °C | 490 - 610 MPa Show Material materials with Resistencia a la tracción of 490 - 610 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | -100.0 °C | 423 J/(kg·K) Show Material materials with Calor específico of 423 J/(kg·K) | |
20.0 °C | 461 J/(kg·K) Show Material materials with Calor específico of 461 J/(kg·K) | ||
100.0 °C | 479 J/(kg·K) Show Material materials with Calor específico of 479 J/(kg·K) | ||
200.0 °C | 499 J/(kg·K) Show Material materials with Calor específico of 499 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) Show Material materials with Calor específico of 517 J/(kg·K) | ||
400.0 °C | 536 J/(kg·K) Show Material materials with Calor específico of 536 J/(kg·K) | ||
500.0 °C | 558 J/(kg·K) Show Material materials with Calor específico of 558 J/(kg·K) | ||
600.0 °C | 587 J/(kg·K) Show Material materials with Calor específico of 587 J/(kg·K) | ||
Coeficiente de dilatación térmica | -100.0 °C | 1.08E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.08E-5 1/K | |
20.0 °C | 1.19E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.19E-5 1/K | ||
100.0 °C | 1.11E-5 - 1.25E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.11E-5 - 1.25E-5 1/K | ||
200.0 °C | 1.21E-5 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.21E-5 - 1.3E-5 1/K | ||
300.0 °C | 1.29E-5 - 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29E-5 - 1.36E-5 1/K | ||
400.0 °C | 1.35E-5 - 1.41E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 - 1.41E-5 1/K | ||
500.0 °C | 1.39E-5 - 1.45E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.39E-5 - 1.45E-5 1/K | ||
600.0 °C | 1.41E-5 - 1.49E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.41E-5 - 1.49E-5 1/K | ||
Conductividad térmica | 20.0 °C | 39.6 W/(m·K) Show Material materials with Conductividad térmica of 39.6 W/(m·K) | |
100.0 °C | 41 W/(m·K) Show Material materials with Conductividad térmica of 41 W/(m·K) | ||
200.0 °C | 41 W/(m·K) Show Material materials with Conductividad térmica of 41 W/(m·K) | ||
300.0 °C | 39.9 W/(m·K) Show Material materials with Conductividad térmica of 39.9 W/(m·K) | ||
400.0 °C | 38.1 W/(m·K) Show Material materials with Conductividad térmica of 38.1 W/(m·K) | ||
500.0 °C | 35.9 W/(m·K) Show Material materials with Conductividad térmica of 35.9 W/(m·K) | ||
600.0 °C | 33.6 W/(m·K) Show Material materials with Conductividad térmica of 33.6 W/(m·K) | ||
Difusividad térmica | 20.0 °C | 11 mm²/s Show Material materials with Difusividad térmica of 11 mm²/s | |
100.0 °C | 10.6 mm²/s Show Material materials with Difusividad térmica of 10.6 mm²/s | ||
200.0 °C | 9.9 mm²/s Show Material materials with Difusividad térmica of 9.9 mm²/s | ||
300.0 °C | 9 mm²/s Show Material materials with Difusividad térmica of 9 mm²/s | ||
400.0 °C | 8.1 mm²/s Show Material materials with Difusividad térmica of 8.1 mm²/s | ||
500.0 °C | 6.9 mm²/s Show Material materials with Difusividad térmica of 6.9 mm²/s | ||
600.0 °C | 5.7 mm²/s Show Material materials with Difusividad térmica of 5.7 mm²/s | ||
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 2.63E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.63E-7 Ω·m |
100.0 °C | 3.12E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.12E-7 Ω·m | |
200.0 °C | 3.85E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.85E-7 Ω·m | |
300.0 °C | 4.7E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.7E-7 Ω·m | |
400.0 °C | 5.71E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.71E-7 Ω·m | |
500.0 °C | 6.88E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.88E-7 Ω·m | |
600.0 °C | 8.25E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.25E-7 Ω·m | |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.015 - 0.05 % Show Material materials with Aluminio of 0.015 - 0.05 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.17 - 0.23 % Show Material materials with Carbono of 0.17 - 0.23 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 - 1.5 % Show Material materials with Manganeso of 1 - 1.5 % |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % |