General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.87 g/cm³ Show Material materials with Densidad of 7.87 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Elongación | 20.0 °C | 18 % Show Material materials with Elongación of 18 % | |
Límite elástico | 20.0 °C | 480 - 490 MPa Show Material materials with Límite elástico of 480 - 490 MPa | |
Módulo elástico | -100.0 °C | 209 GPa Show Material materials with Módulo elástico of 209 GPa | |
20.0 °C | 203 GPa Show Material materials with Módulo elástico of 203 GPa | ||
100.0 °C | 198 GPa Show Material materials with Módulo elástico of 198 GPa | ||
200.0 °C | 191 GPa Show Material materials with Módulo elástico of 191 GPa | ||
300.0 °C | 183 GPa Show Material materials with Módulo elástico of 183 GPa | ||
400.0 °C | 175 GPa Show Material materials with Módulo elástico of 175 GPa | ||
Resistencia a la tracción | 20.0 °C | 640 - 840 MPa Show Material materials with Resistencia a la tracción of 640 - 840 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | -100.0 °C | 420 J/(kg·K) Show Material materials with Calor específico of 420 J/(kg·K) | |
20.0 °C | 463 J/(kg·K) Show Material materials with Calor específico of 463 J/(kg·K) | ||
100.0 °C | 478 J/(kg·K) Show Material materials with Calor específico of 478 J/(kg·K) | ||
200.0 °C | 494 J/(kg·K) Show Material materials with Calor específico of 494 J/(kg·K) | ||
300.0 °C | 510 J/(kg·K) Show Material materials with Calor específico of 510 J/(kg·K) | ||
400.0 °C | 528 J/(kg·K) Show Material materials with Calor específico of 528 J/(kg·K) | ||
Coeficiente de dilatación térmica | -100.0 °C | 1.08E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.08E-5 1/K | |
20.0 °C | 1.19E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.19E-5 1/K | ||
100.0 °C | 1.23E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.23E-5 1/K | ||
200.0 °C | 1.28E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.28E-5 1/K | ||
300.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | ||
400.0 °C | 1.35E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 1/K | ||
Conductividad térmica | -100.0 °C | 25.6 W/(m·K) Show Material materials with Conductividad térmica of 25.6 W/(m·K) | |
20.0 °C | 32 W/(m·K) Show Material materials with Conductividad térmica of 32 W/(m·K) | ||
100.0 °C | 34.4 W/(m·K) Show Material materials with Conductividad térmica of 34.4 W/(m·K) | ||
200.0 °C | 35.7 W/(m·K) Show Material materials with Conductividad térmica of 35.7 W/(m·K) | ||
300.0 °C | 35.9 W/(m·K) Show Material materials with Conductividad térmica of 35.9 W/(m·K) | ||
400.0 °C | 34.8 W/(m·K) Show Material materials with Conductividad térmica of 34.8 W/(m·K) | ||
Difusividad térmica | -100.0 °C | 8.7 mm²/s Show Material materials with Difusividad térmica of 8.7 mm²/s | |
20.0 °C | 8.8 mm²/s Show Material materials with Difusividad térmica of 8.8 mm²/s | ||
100.0 °C | 9 mm²/s Show Material materials with Difusividad térmica of 9 mm²/s | ||
200.0 °C | 8.7 mm²/s Show Material materials with Difusividad térmica of 8.7 mm²/s | ||
300.0 °C | 8.3 mm²/s Show Material materials with Difusividad térmica of 8.3 mm²/s | ||
400.0 °C | 7.5 mm²/s Show Material materials with Difusividad térmica of 7.5 mm²/s | ||
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | -100.0 °C | 2.31E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.31E-7 Ω·m |
20.0 °C | 3.01E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.01E-7 Ω·m | |
100.0 °C | 3.51E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.51E-7 Ω·m | |
200.0 °C | 4.19E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.19E-7 Ω·m | |
300.0 °C | 4.95E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.95E-7 Ω·m | |
400.0 °C | 5.91E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.91E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.6 - 1.4 % Show Material materials with Manganeso of 0.6 - 1.4 % |
Molibdeno | 0.2 - 0.35 % Show Material materials with Molibdeno of 0.2 - 0.35 % |
Níquel | 5 - 6 % Show Material materials with Níquel of 5 - 6 % |
Silicona | 0.35 % Show Material materials with Silicona of 0.35 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |