General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.3 g/cm³ Show Material materials with Densidad of 7.3 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.26 [-] Show Material materials with Coeficiente de Poisson of 0.26 [-] | |
Dureza Brinell | 20.0 °C | 275 - 285 [-] Show Material materials with Dureza Brinell of 275 - 285 [-] | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 20.0 °C | 123 - 143 GPa Show Material materials with Módulo elástico of 123 - 143 GPa | |
Plane-Strain Fracture Toughnes | 20.0 °C | 20.6 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 20.6 MPa·√m | |
Resistencia a la tracción | 20.0 °C | 210 - 450 MPa Show Material materials with Resistencia a la tracción of 210 - 450 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 200.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
600.0 °C | 535 J/(kg·K) Show Material materials with Calor específico of 535 J/(kg·K) | ||
Conductividad térmica | 23.0 °C | 55 W/(m·K) Show Material materials with Conductividad térmica of 55 W/(m·K) | Typical for Cast Iron |
Temperatura de fusión | 1120 °C Show Material materials with Temperatura de fusión of 1120 °C | Typical for Cast Iron |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 6.7E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.7E-7 Ω·m |