General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.75 g/cm³ Show Material materials with Densidad of 7.75 g/cm³ | Typical for Iron Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.28 [-] Show Material materials with Coeficiente de Poisson of 0.28 [-] | Typical for Iron Alloy |
Dureza Brinell | 20.0 °C | 140 - 250 [-] Show Material materials with Dureza Brinell of 140 - 250 [-] | |
Elongación | 20.0 °C | 2 % Show Material materials with Elongación of 2 % | |
Módulo elástico | 23.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | Typical for Iron Alloy |
Resistencia a la tracción | 20.0 °C | 190 - 280 MPa Show Material materials with Resistencia a la tracción of 190 - 280 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 2E-5 1/K | Typical for Iron Alloy |
Chemical properties
Property | Value |
---|---|
Carbono | 2.5 % Show Material materials with Carbono of 2.5 % |
Cromo | 1.5 - 4.5 % Show Material materials with Cromo of 1.5 - 4.5 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Níquel | 18 - 22 % Show Material materials with Níquel of 18 - 22 % |
Silicona | 3.5 - 5.5 % Show Material materials with Silicona of 3.5 - 5.5 % |