General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.75 g/cm³ Show Material materials with Densidad of 7.75 g/cm³ | Typical for Iron Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.28 [-] Show Material materials with Coeficiente de Poisson of 0.28 [-] | Typical for Iron Alloy |
Dureza Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Dureza Brinell of 120 - 150 [-] | |
Elongación | 20.0 °C | 15 % Show Material materials with Elongación of 15 % | |
Límite elástico | 20.0 °C | 210 - 260 MPa Show Material materials with Límite elástico of 210 - 260 MPa | |
Módulo elástico | 23.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | Typical for Iron Alloy |
Resistencia a la tracción | 20.0 °C | 390 - 470 MPa Show Material materials with Resistencia a la tracción of 390 - 470 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 2E-5 1/K | Typical for Iron Alloy |
Chemical properties
Property | Value |
---|---|
Carbono | 3 % Show Material materials with Carbono of 3 % |
Fósforo | 0.08 % Show Material materials with Fósforo of 0.08 % |
Manganeso | 6 - 7 % Show Material materials with Manganeso of 6 - 7 % |
Níquel | 12 - 14 % Show Material materials with Níquel of 12 - 14 % |
Silicona | 2 - 3 % Show Material materials with Silicona of 2 - 3 % |