General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Densidad of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | Typical for Cast Iron |
Dureza Brinell | 20.0 °C | 150 - 255 [-] Show Material materials with Dureza Brinell of 150 - 255 [-] | |
Elongación | 20.0 °C | 7 % Show Material materials with Elongación of 7 % | |
Límite elástico | 20.0 °C | 210 - 260 MPa Show Material materials with Límite elástico of 210 - 260 MPa | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 23.0 °C | 152 GPa Show Material materials with Módulo elástico of 152 GPa | Typical for Cast Iron |
Resistencia a la tracción | 20.0 °C | 390 - 500 MPa Show Material materials with Resistencia a la tracción of 390 - 500 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Calor específico of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Conductividad térmica | 23.0 °C | 55 W/(m·K) Show Material materials with Conductividad térmica of 55 W/(m·K) | Typical for Cast Iron |
Temperatura de fusión | 1120 °C Show Material materials with Temperatura de fusión of 1120 °C | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Carbono | 3 % Show Material materials with Carbono of 3 % |
Cromo | 2.5 - 3.5 % Show Material materials with Cromo of 2.5 - 3.5 % |
Fósforo | 0.08 % Show Material materials with Fósforo of 0.08 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Níquel | 18 - 22 % Show Material materials with Níquel of 18 - 22 % |
Silicona | 1.5 - 3 % Show Material materials with Silicona of 1.5 - 3 % |