General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.15 g/cm³ Show Material materials with Densidad of 7.15 g/cm³ | Typical for Ductile (Nodular) Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.26 - 0.31 [-] Show Material materials with Coeficiente de Poisson of 0.26 - 0.31 [-] | Typical for Ductile (Nodular) Cast Iron |
Dureza Brinell | 20.0 °C | 210 - 260 [-] Show Material materials with Dureza Brinell of 210 - 260 [-] | |
Elongación | 20.0 °C | 2 % Show Material materials with Elongación of 2 % | |
Límite elástico | 20.0 °C | 430 MPa Show Material materials with Límite elástico of 430 MPa | |
Módulo de cizallamiento | 23.0 °C | 63 - 66 GPa Show Material materials with Módulo de cizallamiento of 63 - 66 GPa | Typical for Ductile (Nodular) Cast Iron |
Módulo elástico | 23.0 °C | 165 - 180 GPa Show Material materials with Módulo elástico of 165 - 180 GPa | Typical for Ductile (Nodular) Cast Iron |
Resistencia a la tracción | 20.0 °C | 650 MPa Show Material materials with Resistencia a la tracción of 650 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 - 502 J/(kg·K) Show Material materials with Calor específico of 460 - 502 J/(kg·K) | Typical for Ductile (Nodular) Cast Iron |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.6E-5 1/K | Typical for Ductile (Nodular) Cast Iron |
Conductividad térmica | 23.0 °C | 13 - 42 W/(m·K) Show Material materials with Conductividad térmica of 13 - 42 W/(m·K) | Typical for Ductile (Nodular) Cast Iron |
Temperatura de fusión | 1150 - 1200 °C Show Material materials with Temperatura de fusión of 1150 - 1200 °C | Typical for Ductile (Nodular) Cast Iron |
Chemical properties
Property | Value |
---|---|
Azufre | 0.1 - 0.15 % Show Material materials with Azufre of 0.1 - 0.15 % |
Carbono | 2.3 - 2.6 % Show Material materials with Carbono of 2.3 - 2.6 % |
Manganeso | 0.4 - 0.5 % Show Material materials with Manganeso of 0.4 - 0.5 % |
Silicona | 1.2 - 1.5 % Show Material materials with Silicona of 1.2 - 1.5 % |