General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.2 - 7.34 g/cm³ Show Material materials with Densidad of 7.2 - 7.34 g/cm³ | Typical for Malleable Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | Typical for Malleable Cast Iron |
Dureza Brinell | 20.0 °C | 220 [-] Show Material materials with Dureza Brinell of 220 [-] | |
Elongación | 20.0 °C | 4 - 10 % Show Material materials with Elongación of 4 - 10 % | |
Límite elástico | 20.0 °C | 230 - 280 MPa Show Material materials with Límite elástico of 230 - 280 MPa | |
Módulo de cizallamiento | 23.0 °C | 64 GPa Show Material materials with Módulo de cizallamiento of 64 GPa | Typical for Malleable Cast Iron |
Módulo elástico | 23.0 °C | 165 - 180 GPa Show Material materials with Módulo elástico of 165 - 180 GPa | Typical for Malleable Cast Iron |
Resistencia a la tracción | 20.0 °C | 400 - 480 MPa Show Material materials with Resistencia a la tracción of 400 - 480 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Calor específico of 460 - 527 J/(kg·K) | Typical for Malleable Cast Iron |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.4E-5 1/K | Typical for Malleable Cast Iron |
Conductividad térmica | 23.0 °C | 51 W/(m·K) Show Material materials with Conductividad térmica of 51 W/(m·K) | Typical for Malleable Cast Iron |
Temperatura de fusión | 1120 °C Show Material materials with Temperatura de fusión of 1120 °C | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Azufre | 0.12 - 0.25 % Show Material materials with Azufre of 0.12 - 0.25 % |
Carbono | 3 - 3.4 % Show Material materials with Carbono of 3 - 3.4 % |
Manganeso | 0.4 - 0.6 % Show Material materials with Manganeso of 0.4 - 0.6 % |
Silicona | 0.4 - 0.8 % Show Material materials with Silicona of 0.4 - 0.8 % |