General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.84 g/cm³ Show Material materials with Densidad of 7.84 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 14 % Show Material materials with Elongación of 14 % | |
Elongación transversal | 20.0 °C | 16 % Show Material materials with Elongación transversal of 16 % | |
Límite elástico | 20.0 °C | 690 MPa Show Material materials with Límite elástico of 690 MPa | |
Límite elástico transversal | 20.0 °C | 690 MPa Show Material materials with Límite elástico transversal of 690 MPa | |
Módulo elástico | 20.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | |
Resistencia a la tracción | 20.0 °C | 760 - 900 MPa Show Material materials with Resistencia a la tracción of 760 - 900 MPa | |
Resistencia a la tracción transversal | 20.0 °C | 760 - 900 MPa Show Material materials with Resistencia a la tracción transversal of 760 - 900 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 430 J/(kg·K) Show Material materials with Calor específico of 430 J/(kg·K) |
Coeficiente de dilatación térmica | 100.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K |
Conductividad térmica | 20.0 °C | 38 W/(m·K) Show Material materials with Conductividad térmica of 38 W/(m·K) |
Temperatura máx. de funcionamiento, largo | -50 - 0 °C Show Material materials with Temperatura máx. de funcionamiento, largo of -50 - 0 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 2.8E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.8E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Boro | 5E-4 % Show Material materials with Boro of 5E-4 % |
Carbono | 0.12 - 0.2 % Show Material materials with Carbono of 0.12 - 0.2 % |
Cromo | 0.4 - 0.65 % Show Material materials with Cromo of 0.4 - 0.65 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.7 - 1 % Show Material materials with Manganeso of 0.7 - 1 % |
Molibdeno | 0.15 - 0.25 % Show Material materials with Molibdeno of 0.15 - 0.25 % |
Silicona | 0.2 - 0.35 % Show Material materials with Silicona of 0.2 - 0.35 % |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % |
Vanadio | 0.03 - 0.08 % Show Material materials with Vanadio of 0.03 - 0.08 % |