General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.7 - 7.77 g/cm³ Show Material materials with Densidad of 7.7 - 7.77 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] |
Dureza Brinell | 20.0 °C | 180 [-] Show Material materials with Dureza Brinell of 180 [-] |
Elongación | 20.0 °C | 20 % Show Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 20.0 °C | 320 MPa Show Material materials with Límite elástico Rp 0,2 of 320 MPa |
50.0 °C | 310 MPa Show Material materials with Límite elástico Rp 0,2 of 310 MPa | |
100.0 °C | 240 MPa Show Material materials with Límite elástico Rp 0,2 of 240 MPa | |
150.0 °C | 235 MPa Show Material materials with Límite elástico Rp 0,2 of 235 MPa | |
200.0 °C | 230 MPa Show Material materials with Límite elástico Rp 0,2 of 230 MPa | |
250.0 °C | 220 MPa Show Material materials with Límite elástico Rp 0,2 of 220 MPa | |
300.0 °C | 215 MPa Show Material materials with Límite elástico Rp 0,2 of 215 MPa | |
Módulo de cizallamiento | 20.0 °C | 81.7 GPa Show Material materials with Módulo de cizallamiento of 81.7 GPa |
Módulo elástico | 20.0 °C | 211.67 - 220 GPa Show Material materials with Módulo elástico of 211.67 - 220 GPa |
100.0 °C | 213 - 216 GPa Show Material materials with Módulo elástico of 213 - 216 GPa | |
200.0 °C | 206 - 209 GPa Show Material materials with Módulo elástico of 206 - 209 GPa | |
300.0 °C | 198 - 200 GPa Show Material materials with Módulo elástico of 198 - 200 GPa | |
400.0 °C | 190 - 192 GPa Show Material materials with Módulo elástico of 190 - 192 GPa | |
500.0 °C | 180 - 183 GPa Show Material materials with Módulo elástico of 180 - 183 GPa | |
600.0 °C | 167 GPa Show Material materials with Módulo elástico of 167 GPa | |
700.0 °C | 150 GPa Show Material materials with Módulo elástico of 150 GPa | |
Resistencia a la tracción | 20.0 °C | 450 - 600 MPa Show Material materials with Resistencia a la tracción of 450 - 600 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 429 - 430 J/(kg·K) Show Material materials with Calor específico of 429 - 430 J/(kg·K) | |
100.0 °C | 464 J/(kg·K) Show Material materials with Calor específico of 464 J/(kg·K) | ||
200.0 °C | 492 J/(kg·K) Show Material materials with Calor específico of 492 J/(kg·K) | ||
300.0 °C | 511 J/(kg·K) Show Material materials with Calor específico of 511 J/(kg·K) | ||
400.0 °C | 531 J/(kg·K) Show Material materials with Calor específico of 531 J/(kg·K) | ||
500.0 °C | 554 J/(kg·K) Show Material materials with Calor específico of 554 J/(kg·K) | ||
600.0 °C | 585 J/(kg·K) Show Material materials with Calor específico of 585 J/(kg·K) | ||
700.0 °C | 626 J/(kg·K) Show Material materials with Calor específico of 626 J/(kg·K) | ||
Coeficiente de dilatación térmica | -100.0 °C | 1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 1/K | |
20.0 °C | 1.08E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.08E-5 1/K | ||
100.0 °C | 1.04E-5 - 1.13E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.04E-5 - 1.13E-5 1/K | ||
200.0 °C | 1.08E-5 - 1.18E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.08E-5 - 1.18E-5 1/K | ||
300.0 °C | 1.12E-5 - 1.23E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.12E-5 - 1.23E-5 1/K | ||
400.0 °C | 1.16E-5 - 1.27E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.16E-5 - 1.27E-5 1/K | ||
500.0 °C | 1.19E-5 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.19E-5 - 1.3E-5 1/K | ||
600.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | ||
700.0 °C | 1.33E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.33E-5 1/K | ||
Conductividad térmica | 20.0 °C | 20.7 - 25 W/(m·K) Show Material materials with Conductividad térmica of 20.7 - 25 W/(m·K) | |
100.0 °C | 22.6 W/(m·K) Show Material materials with Conductividad térmica of 22.6 W/(m·K) | ||
200.0 °C | 24.4 W/(m·K) Show Material materials with Conductividad térmica of 24.4 W/(m·K) | ||
300.0 °C | 25.8 W/(m·K) Show Material materials with Conductividad térmica of 25.8 W/(m·K) | ||
400.0 °C | 26.9 W/(m·K) Show Material materials with Conductividad térmica of 26.9 W/(m·K) | ||
500.0 °C | 27.8 W/(m·K) Show Material materials with Conductividad térmica of 27.8 W/(m·K) | ||
600.0 °C | 28.5 W/(m·K) Show Material materials with Conductividad térmica of 28.5 W/(m·K) | ||
700.0 °C | 28.8 W/(m·K) Show Material materials with Conductividad térmica of 28.8 W/(m·K) | ||
Difusividad térmica | 20.0 °C | 6.2 mm²/s Show Material materials with Difusividad térmica of 6.2 mm²/s | |
100.0 °C | 5.9 mm²/s Show Material materials with Difusividad térmica of 5.9 mm²/s | ||
200.0 °C | 6 mm²/s Show Material materials with Difusividad térmica of 6 mm²/s | ||
300.0 °C | 6 mm²/s Show Material materials with Difusividad térmica of 6 mm²/s | ||
400.0 °C | 5.7 mm²/s Show Material materials with Difusividad térmica of 5.7 mm²/s | ||
500.0 °C | 5.4 mm²/s Show Material materials with Difusividad térmica of 5.4 mm²/s | ||
600.0 °C | 4.8 mm²/s Show Material materials with Difusividad térmica of 4.8 mm²/s | ||
700.0 °C | 4 mm²/s Show Material materials with Difusividad térmica of 4 mm²/s | ||
Temperatura de fusión | 1425 - 1530 °C Show Material materials with Temperatura de fusión of 1425 - 1530 °C | Typical for Ferritic Stainless Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 5.03E-7 - 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.03E-7 - 6E-7 Ω·m |
100.0 °C | 5.67E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.67E-7 Ω·m | |
200.0 °C | 6.47E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.47E-7 Ω·m | |
300.0 °C | 7.27E-7 Ω·m Show Material materials with Resistividad eléctrica of 7.27E-7 Ω·m | |
400.0 °C | 8.09E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.09E-7 Ω·m | |
500.0 °C | 8.9E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.9E-7 Ω·m | |
600.0 °C | 9.72E-7 Ω·m Show Material materials with Resistividad eléctrica of 9.72E-7 Ω·m | |
700.0 °C | 1.06E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.06E-6 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cromo | 10.5 - 12.5 % Show Material materials with Cromo of 10.5 - 12.5 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Nitrógeno | 0.03 % Show Material materials with Nitrógeno of 0.03 % |
Níquel | 0.3 - 1 % Show Material materials with Níquel of 0.3 - 1 % |