General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.7 g/cm³ Show Material materials with Densidad of 7.7 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Dureza Brinell | 20.0 °C | 230 [-] Show Material materials with Dureza Brinell of 230 [-] | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Martensitic Stainless Steel |
Módulo elástico | 20.0 °C | 223 GPa Show Material materials with Módulo elástico of 223 GPa | |
100.0 °C | 217 GPa Show Material materials with Módulo elástico of 217 GPa | ||
200.0 °C | 209 GPa Show Material materials with Módulo elástico of 209 GPa | ||
300.0 °C | 201 GPa Show Material materials with Módulo elástico of 201 GPa | ||
400.0 °C | 192 GPa Show Material materials with Módulo elástico of 192 GPa | ||
500.0 °C | 183 GPa Show Material materials with Módulo elástico of 183 GPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 430 J/(kg·K) Show Material materials with Calor específico of 430 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.04E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.04E-5 1/K | |
200.0 °C | 1.08E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.08E-5 1/K | ||
300.0 °C | 1.12E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.12E-5 1/K | ||
400.0 °C | 1.16E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.16E-5 1/K | ||
500.0 °C | 1.19E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.19E-5 1/K | ||
Conductividad térmica | 20.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) | |
Temperatura de fusión | 1370 - 1530 °C Show Material materials with Temperatura de fusión of 1370 - 1530 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.25 - 0.35 % Show Material materials with Carbono of 0.25 - 0.35 % |
Cromo | 14 - 16 % Show Material materials with Cromo of 14 - 16 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 0.85 - 1.1 % Show Material materials with Molibdeno of 0.85 - 1.1 % |
Nitrógeno | 0.3 - 0.5 % Show Material materials with Nitrógeno of 0.3 - 0.5 % |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |