General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.7 g/cm³ Show Material materials with Densidad of 7.7 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Duplex Stainless Steel |
Dureza Brinell | 20.0 °C | 230 - 300 [-] Show Material materials with Dureza Brinell of 230 - 300 [-] | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Duplex Stainless Steel |
Módulo elástico | 23.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | Typical for Duplex Stainless Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.05E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.05E-5 1/K | |
200.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | ||
300.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | ||
400.0 °C | 1.25E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.25E-5 1/K | ||
Conductividad térmica | 20.0 °C | 17 W/(m·K) Show Material materials with Conductividad térmica of 17 W/(m·K) | |
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Temperatura máx. de funcionamiento | 300 °C Show Material materials with Temperatura máx. de funcionamiento of 300 °C | Typical for Duplex Stainless Steel | |
Temperatura máx. de funcionamiento, largo | 0 - 1100 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 1100 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 8.1E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.1E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.3 - 0.5 % Show Material materials with Carbono of 0.3 - 0.5 % |
Cromo | 26 - 28 % Show Material materials with Cromo of 26 - 28 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Molibdeno | 2 - 2.5 % Show Material materials with Molibdeno of 2 - 2.5 % |
Níquel | 4 - 6 % Show Material materials with Níquel of 4 - 6 % |
Silicona | 2 % Show Material materials with Silicona of 2 % |