Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Elongación | 20.0 °C | 16 % Show Material materials with Elongación of 16 % | |
Límite elástico | 20.0 °C | 400 - 450 MPa Show Material materials with Límite elástico of 400 - 450 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 550 - 750 MPa Show Material materials with Resistencia a la tracción of 550 - 750 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 335 - 481 J/(kg·K) Show Material materials with Calor específico of 335 - 481 J/(kg·K) | Typical for Nickel Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 9E-6 - 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9E-6 - 1.3E-5 1/K | Typical for Nickel Molybdenum Steel |
Conductividad térmica | 23.0 °C | 44 W/(m·K) Show Material materials with Conductividad térmica of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.17 - 0.23 % Show Material materials with Carbono of 0.17 - 0.23 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 1.2 - 1.5 % Show Material materials with Manganeso of 1.2 - 1.5 % |
Molibdeno | 0.45 - 0.6 % Show Material materials with Molibdeno of 0.45 - 0.6 % |
Níquel | 0.5 - 0.8 % Show Material materials with Níquel of 0.5 - 0.8 % |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % |