General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Elongación | 20.0 °C | 16 % Show Material materials with Elongación of 16 % | |
Límite elástico | 20.0 °C | 550 MPa Show Material materials with Límite elástico of 550 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 650 - 800 MPa Show Material materials with Resistencia a la tracción of 650 - 800 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 448 - 670 J/(kg·K) Show Material materials with Calor específico of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | -196.0 °C | 8.6E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.6E-6 1/K | |
-170.0 °C | 9.4E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 9.4E-6 1/K | ||
-120.0 °C | 1.03E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.03E-5 1/K | ||
-50.0 °C | 1.12E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.12E-5 1/K | ||
-25.0 °C | 1.14E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.14E-5 1/K | ||
Conductividad térmica | -20.0 °C | 35 W/(m·K) Show Material materials with Conductividad térmica of 35 W/(m·K) | |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.12 - 0.16 % Show Material materials with Carbono of 0.12 - 0.16 % |
Cromo | 1.3 - 1.8 % Show Material materials with Cromo of 1.3 - 1.8 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Manganeso | 0.55 - 0.7 % Show Material materials with Manganeso of 0.55 - 0.7 % |
Molibdeno | 0.45 - 0.55 % Show Material materials with Molibdeno of 0.45 - 0.55 % |
Níquel | 2.7 - 3 % Show Material materials with Níquel of 2.7 - 3 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |