General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación transversal | 20.0 °C | 12 - 13 % Show Material materials with Elongación transversal of 12 - 13 % | |
Límite elástico Rp 0,2 | 100.0 °C | 585 MPa Show Material materials with Límite elástico Rp 0,2 of 585 MPa | |
200.0 °C | 560 MPa Show Material materials with Límite elástico Rp 0,2 of 560 MPa | ||
250.0 °C | 550 MPa Show Material materials with Límite elástico Rp 0,2 of 550 MPa | ||
300.0 °C | 535 MPa Show Material materials with Límite elástico Rp 0,2 of 535 MPa | ||
350.0 °C | 520 MPa Show Material materials with Límite elástico Rp 0,2 of 520 MPa | ||
400.0 °C | 500 MPa Show Material materials with Límite elástico Rp 0,2 of 500 MPa | ||
450.0 °C | 480 MPa Show Material materials with Límite elástico Rp 0,2 of 480 MPa | ||
500.0 °C | 440 MPa Show Material materials with Límite elástico Rp 0,2 of 440 MPa | ||
Límite elástico transversal Rp 0,2 | 20.0 °C | 560 - 700 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 560 - 700 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Reducción de área, transversal | 20.0 °C | 40 % Show Material materials with Reducción de área, transversal of 40 % | |
Resistencia a la tracción transversal | 20.0 °C | 650 - 930 MPa Show Material materials with Resistencia a la tracción transversal of 650 - 930 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Azufre | 7E-3 % Show Material materials with Azufre of 7E-3 % |
Carbono | 0.2 - 0.24 % Show Material materials with Carbono of 0.2 - 0.24 % |
Cromo | 2 - 2.2 % Show Material materials with Cromo of 2 - 2.2 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Manganeso | 0.6 - 0.8 % Show Material materials with Manganeso of 0.6 - 0.8 % |
Molibdeno | 0.8 - 0.9 % Show Material materials with Molibdeno of 0.8 - 0.9 % |
Níquel | 0.7 - 0.8 % Show Material materials with Níquel of 0.7 - 0.8 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Vanadio | 0.25 - 0.35 % Show Material materials with Vanadio of 0.25 - 0.35 % |
Wolframio | 0.6 - 0.7 % Show Material materials with Wolframio of 0.6 - 0.7 % |