General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 11 % Show Material materials with Elongación of 11 % | |
Límite elástico | 20.0 °C | 520 MPa Show Material materials with Límite elástico of 520 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 736 MPa Show Material materials with Resistencia a la tracción of 736 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.46 - 0.54 % Show Material materials with Carbono of 0.46 - 0.54 % |
Cromo | 0.9 - 1.2 % Show Material materials with Cromo of 0.9 - 1.2 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Silicona | 0.25 - 0.5 % Show Material materials with Silicona of 0.25 - 0.5 % |
Vanadio | 0.07 - 0.12 % Show Material materials with Vanadio of 0.07 - 0.12 % |