General
Property | Value | Comment |
---|---|---|
Densidad | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ | Typical for Nickel Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.291 [-] Show Material materials with Coeficiente de Poisson of 0.291 [-] | Typical for Nickel Steel | ||||
Elongación | 20 °C | 18 % Show Material materials with Elongación of 18 % | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat | |
Límite elástico | 20 °C | 585 MPa Show Material materials with Límite elástico of 585 MPa | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat | |
Módulo de cizallamiento | 76 GPa Show Material materials with Módulo de cizallamiento of 76 GPa | Typical for Nickel Steel | ||||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Steel | ||||
Resistencia a la tracción | 20 °C | 680 - 820 MPa Show Material materials with Resistencia a la tracción of 680 - 820 MPa | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Nickel Steel |
Conductividad térmica | 10 - 50 W/(m·K) Show Material materials with Conductividad térmica of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Temperatura de fusión | 1316 - 1595 °C Show Material materials with Temperatura de fusión of 1316 - 1595 °C | Typical for Nickel Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.005 % Show Material materials with Azufre of 0.005 % | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat |
Fósforo | 0.015 % Show Material materials with Fósforo of 0.015 % | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat |
Manganeso | 0.3 - 0.8 % Show Material materials with Manganeso of 0.3 - 0.8 % | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat |
Níquel | 8.5 - 10 % Show Material materials with Níquel of 8.5 - 10 % | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat |
Silicona | 0.35 % Show Material materials with Silicona of 0.35 % | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat |
Vanadio | 0.01 % Show Material materials with Vanadio of 0.01 % | normalized, normalized and tempered (+N+NT) | EN 10028-4 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |