General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | ||||
Dureza Brinell | 263 [-] Show Material materials with Dureza Brinell of 263 [-] | Predicted Value, Transverse | ||||
Elongación | 19.7 % Show Material materials with Elongación of 19.7 % | Predicted Value, A200 | ||||
20.3 % Show Material materials with Elongación of 20.3 % | Predicted Value, Transverse | |||||
21.5 % Show Material materials with Elongación of 21.5 % | Predicted Value, A5 | |||||
24.9 % Show Material materials with Elongación of 24.9 % | Predicted Value, A80 Transverse | |||||
27.8 % Show Material materials with Elongación of 27.8 % | Predicted Value, A50 | |||||
31.8 % Show Material materials with Elongación of 31.8 % | Predicted Value | |||||
20 °C | 28 % Show Material materials with Elongación of 28 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | A80 | |
Estricción | 43.3 % Show Material materials with Estricción of 43.3 % | Predicted Value, Transverse | ||||
44.8 % Show Material materials with Estricción of 44.8 % | Predicted Value | |||||
Límite elástico | 257.3 MPa Show Material materials with Límite elástico of 257.3 MPa | Predicted Value, RP1 | ||||
258.4 MPa Show Material materials with Límite elástico of 258.4 MPa | Predicted Value, RP05 | |||||
284.1 MPa Show Material materials with Límite elástico of 284.1 MPa | Predicted Value, Transverse | |||||
309.1 MPa Show Material materials with Límite elástico of 309.1 MPa | Predicted Value, RP02 | |||||
315 MPa Show Material materials with Límite elástico of 315 MPa | Predicted Value, RP1 Transverse | |||||
455.1 MPa Show Material materials with Límite elástico of 455.1 MPa | Predicted Value, RP02 Transverse | |||||
489.2 MPa Show Material materials with Límite elástico of 489.2 MPa | Predicted Value, RP002 | |||||
20 °C | 140 - 280 MPa Show Material materials with Límite elástico of 140 - 280 MPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | ||||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Resistencia a la tracción | 20 °C | 270 - 410 MPa Show Material materials with Resistencia a la tracción of 270 - 410 MPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | |
Resistencia al cizallamiento | 526.2 MPa Show Material materials with Resistencia al cizallamiento of 526.2 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 327.5 °C Show Material materials with Temperatura máx. de funcionamiento of 327.5 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 8 S/m Show Material materials with Conductividad eléctrica of 8 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.045 % Show Material materials with Azufre of 0.045 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Fósforo | 0.045 % Show Material materials with Fósforo of 0.045 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Manganeso | 0.6 % Show Material materials with Manganeso of 0.6 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |