General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | ||||
Dureza Brinell | 240 [-] Show Material materials with Dureza Brinell of 240 [-] | Predicted Value, Transverse | ||||
Elongación | 16.5 % Show Material materials with Elongación of 16.5 % | Predicted Value, A200 | ||||
18.9 % Show Material materials with Elongación of 18.9 % | Predicted Value, Transverse | |||||
19.4 % Show Material materials with Elongación of 19.4 % | Predicted Value, A80 Transverse | |||||
21.6 % Show Material materials with Elongación of 21.6 % | Predicted Value, A50 | |||||
21.9 % Show Material materials with Elongación of 21.9 % | Predicted Value | |||||
24.1 % Show Material materials with Elongación of 24.1 % | Predicted Value, A5 | |||||
20 °C | 19 % Show Material materials with Elongación of 19 % | cold rolled | EN 10326, EN 10346 | Strip | A80 | |
Estricción | 39.2 % Show Material materials with Estricción of 39.2 % | Predicted Value | ||||
43.1 % Show Material materials with Estricción of 43.1 % | Predicted Value, Transverse | |||||
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | ||||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Resistencia a la tracción | 20 °C | 330 MPa Show Material materials with Resistencia a la tracción of 330 MPa | cold rolled | EN 10326, EN 10346 | Strip | |
Resistencia al cizallamiento | 499.5 MPa Show Material materials with Resistencia al cizallamiento of 499.5 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 310.4 °C Show Material materials with Temperatura máx. de funcionamiento of 310.4 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 8 S/m Show Material materials with Conductividad eléctrica of 8 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.045 % Show Material materials with Azufre of 0.045 % | cold rolled | EN 10326, EN 10346 | Strip |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % | cold rolled | EN 10326, EN 10346 | Strip |
Fósforo | 0.1 % Show Material materials with Fósforo of 0.1 % | cold rolled | EN 10326, EN 10346 | Strip |
Manganeso | 1.7 % Show Material materials with Manganeso of 1.7 % | cold rolled | EN 10326, EN 10346 | Strip |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % | cold rolled | EN 10326, EN 10346 | Strip |