Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | ||||
Dureza Brinell | 266 [-] Show Material materials with Dureza Brinell of 266 [-] | Predicted Value, Transverse | ||||
Elongación | 14.4 % Show Material materials with Elongación of 14.4 % | Predicted Value, A200 | ||||
19.9 % Show Material materials with Elongación of 19.9 % | Predicted Value, A5 | |||||
21.7 % Show Material materials with Elongación of 21.7 % | Predicted Value, A50 | |||||
21.7 % Show Material materials with Elongación of 21.7 % | Predicted Value, Transverse | |||||
22.4 % Show Material materials with Elongación of 22.4 % | Predicted Value | |||||
20 °C | 33 % Show Material materials with Elongación of 33 % | skin passed | EN 10152 | Strip | A80 Transverse | |
20 °C | 35 % Show Material materials with Elongación of 35 % | skin passed | EN 10152 | Strip | A80 Transverse | |
20 °C | 37 % Show Material materials with Elongación of 37 % | skin passed | EN 10152 | Strip | A80 Transverse | |
20 °C | 37 % Show Material materials with Elongación of 37 % | skin passed | EN 10152 | Strip, Sheet | A80 | |
Estricción | 42.0 % Show Material materials with Estricción of 42.0 % | Predicted Value | ||||
43.5 % Show Material materials with Estricción of 43.5 % | Predicted Value, Transverse | |||||
Límite elástico | 279.1 MPa Show Material materials with Límite elástico of 279.1 MPa | Predicted Value, RP05 | ||||
286.5 MPa Show Material materials with Límite elástico of 286.5 MPa | Predicted Value, RP1 Transverse | |||||
293.2 MPa Show Material materials with Límite elástico of 293.2 MPa | Predicted Value, RP1 | |||||
364.4 MPa Show Material materials with Límite elástico of 364.4 MPa | Predicted Value, RP02 Transverse | |||||
546.1 MPa Show Material materials with Límite elástico of 546.1 MPa | Predicted Value, RP02 | |||||
627.3 MPa Show Material materials with Límite elástico of 627.3 MPa | Predicted Value, RP002 | |||||
20 °C | 140 - 260 MPa Show Material materials with Límite elástico of 140 - 260 MPa | skin passed | EN 10152 | Strip | Transverse | |
20 °C | 140 - 240 MPa Show Material materials with Límite elástico of 140 - 240 MPa | skin passed | EN 10152 | Strip | Transverse | |
20 °C | 140 - 220 MPa Show Material materials with Límite elástico of 140 - 220 MPa | skin passed | EN 10152 | Strip | Transverse | |
20 °C | 140 - 220 MPa Show Material materials with Límite elástico of 140 - 220 MPa | skin passed | EN 10152 | Strip, Sheet | ||
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | ||||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Resistencia a la tracción | 20 °C | 270 - 350 MPa Show Material materials with Resistencia a la tracción of 270 - 350 MPa | skin passed | EN 10152 | Strip | Transverse |
20 °C | 270 - 350 MPa Show Material materials with Resistencia a la tracción of 270 - 350 MPa | skin passed | EN 10152 | Strip, Sheet | ||
Resistencia al cizallamiento | 562.8 MPa Show Material materials with Resistencia al cizallamiento of 562.8 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 364.5 °C Show Material materials with Temperatura máx. de funcionamiento of 364.5 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 8 S/m Show Material materials with Conductividad eléctrica of 8 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | skin passed | EN 10152 | Strip, Sheet |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % | skin passed | EN 10152 | Strip, Sheet |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | skin passed | EN 10152 | Strip, Sheet |
Manganeso | 0.4 % Show Material materials with Manganeso of 0.4 % | skin passed | EN 10152 | Strip, Sheet |