General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 20 - 22 % Show Material materials with Elongación of 20 - 22 % | |
Elongación A80 | 20.0 °C | 16 - 18 % Show Material materials with Elongación A80 of 16 - 18 % | |
Elongación A80 transversal | 20.0 °C | 14 - 16 % Show Material materials with Elongación A80 transversal of 14 - 16 % | |
Elongación transversal | 20.0 °C | 18 - 20 % Show Material materials with Elongación transversal of 18 - 20 % | |
Límite elástico | 20.0 °C | 315 - 355 MPa Show Material materials with Límite elástico of 315 - 355 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 490 - 680 MPa Show Material materials with Resistencia a la tracción of 490 - 680 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.16 % Show Material materials with Carbono of 0.16 % |
Circonio | 0.15 % Show Material materials with Circonio of 0.15 % |
Cobre | 0.25 - 0.55 % Show Material materials with Cobre of 0.25 - 0.55 % |
Cromo | 0.4 - 0.8 % Show Material materials with Cromo of 0.4 - 0.8 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.5 - 1 % Show Material materials with Manganeso of 0.5 - 1 % |
Molibdeno | 0.3 % Show Material materials with Molibdeno of 0.3 % |
Níquel | 0.65 % Show Material materials with Níquel of 0.65 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |