General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | ||||
Dureza Brinell | 269 [-] Show Material materials with Dureza Brinell of 269 [-] | Predicted Value, Transverse | ||||
Elongación | 14.4 % Show Material materials with Elongación of 14.4 % | Predicted Value, A200 | ||||
19.9 % Show Material materials with Elongación of 19.9 % | Predicted Value, A5 | |||||
21.3 % Show Material materials with Elongación of 21.3 % | Predicted Value, A50 | |||||
21.4 % Show Material materials with Elongación of 21.4 % | Predicted Value, Transverse | |||||
21.6 % Show Material materials with Elongación of 21.6 % | Predicted Value | |||||
20 °C | 34 % Show Material materials with Elongación of 34 % | cold rolled, skin passed | EN 10209 | Sheet | A80 Transverse | |
20 °C | 36 % Show Material materials with Elongación of 36 % | cold rolled, skin passed | EN 10209 | Sheet | A80 Transverse | |
20 °C | 38 % Show Material materials with Elongación of 38 % | cold rolled, skin passed | EN 10209 | Sheet | A80 Transverse | |
20 °C | 38 % Show Material materials with Elongación of 38 % | cold rolled, skin passed | EN 10209 | Strip, Bar | A80 | |
Estricción | 40.5 % Show Material materials with Estricción of 40.5 % | Predicted Value | ||||
43.4 % Show Material materials with Estricción of 43.4 % | Predicted Value, Transverse | |||||
Límite elástico | 286.4 MPa Show Material materials with Límite elástico of 286.4 MPa | Predicted Value, RP1 Transverse | ||||
293.4 MPa Show Material materials with Límite elástico of 293.4 MPa | Predicted Value, RP1 | |||||
331.1 MPa Show Material materials with Límite elástico of 331.1 MPa | Predicted Value, RP05 | |||||
375.9 MPa Show Material materials with Límite elástico of 375.9 MPa | Predicted Value, RP02 Transverse | |||||
548.4 MPa Show Material materials with Límite elástico of 548.4 MPa | Predicted Value, RP02 | |||||
628.3 MPa Show Material materials with Límite elástico of 628.3 MPa | Predicted Value, RP002 | |||||
20 °C | 120 - 230 MPa Show Material materials with Límite elástico of 120 - 230 MPa | cold rolled, skin passed | EN 10209 | Sheet | Transverse | |
20 °C | 120 - 210 MPa Show Material materials with Límite elástico of 120 - 210 MPa | cold rolled, skin passed | EN 10209 | Sheet | Transverse | |
20 °C | 120 - 190 MPa Show Material materials with Límite elástico of 120 - 190 MPa | cold rolled, skin passed | EN 10209 | Sheet | Transverse | |
20 °C | 120 - 190 MPa Show Material materials with Límite elástico of 120 - 190 MPa | cold rolled, skin passed | EN 10209 | Strip, Bar | ||
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | ||||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Resistencia a la tracción | 20 °C | 270 - 350 MPa Show Material materials with Resistencia a la tracción of 270 - 350 MPa | cold rolled, skin passed | EN 10209 | Sheet | Transverse |
20 °C | 270 - 350 MPa Show Material materials with Resistencia a la tracción of 270 - 350 MPa | cold rolled, skin passed | EN 10209 | Strip, Bar | ||
Resistencia al cizallamiento | 563.2 MPa Show Material materials with Resistencia al cizallamiento of 563.2 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 406.7 °C Show Material materials with Temperatura máx. de funcionamiento of 406.7 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 8 S/m Show Material materials with Conductividad eléctrica of 8 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % | cold rolled, skin passed | EN 10209 | Sheet |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % | cold rolled, skin passed | EN 10209 | Sheet |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % | cold rolled, skin passed | EN 10209 | Sheet |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % | cold rolled, skin passed | EN 10209 | Sheet |
Titanio | 0.3 % Show Material materials with Titanio of 0.3 % | cold rolled, skin passed | EN 10209 | Sheet |