General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
20 °C | 7.8 - 7.85 g/cm³ Show Material materials with Densidad of 7.8 - 7.85 g/cm³ | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
20 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Medium Carbon Steel | ||||
Dureza Brinell | 251 [-] Show Material materials with Dureza Brinell of 251 [-] | Predicted Value, Transverse | ||||
20 °C | 207 [-] Show Material materials with Dureza Brinell of 207 [-] | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1, EN 10083-3 | Strip, Sheet, Flat, Bar, Wire, Forging | ||
Módulo de cizallamiento | 20 °C | 81 GPa Show Material materials with Módulo de cizallamiento of 81 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
Módulo elástico | -100 °C | 217 GPa Show Material materials with Módulo elástico of 217 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
20 °C | 210 - 212 GPa Show Material materials with Módulo elástico of 210 - 212 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
20 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
20 °C | 212 GPa Show Material materials with Módulo elástico of 212 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 205 - 207 GPa Show Material materials with Módulo elástico of 205 - 207 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 205 GPa Show Material materials with Módulo elástico of 205 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 207 GPa Show Material materials with Módulo elástico of 207 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 195 - 199 GPa Show Material materials with Módulo elástico of 195 - 199 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 199 GPa Show Material materials with Módulo elástico of 199 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 185 - 192 GPa Show Material materials with Módulo elástico of 185 - 192 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 185 GPa Show Material materials with Módulo elástico of 185 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 192 GPa Show Material materials with Módulo elástico of 192 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
400 °C | 175 - 184 GPa Show Material materials with Módulo elástico of 175 - 184 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
400 °C | 175 GPa Show Material materials with Módulo elástico of 175 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
400 °C | 184 GPa Show Material materials with Módulo elástico of 184 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
500 °C | 175 GPa Show Material materials with Módulo elástico of 175 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
600 °C | 164 GPa Show Material materials with Módulo elástico of 164 GPa | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | -100 °C | 423 J/(kg·K) Show Material materials with Calor específico of 423 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
20 °C | 461 J/(kg·K) Show Material materials with Calor específico of 461 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
20 °C | 461 - 480 J/(kg·K) Show Material materials with Calor específico of 461 - 480 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
20 °C | 480 J/(kg·K) Show Material materials with Calor específico of 480 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 479 J/(kg·K) Show Material materials with Calor específico of 479 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 479 - 500 J/(kg·K) Show Material materials with Calor específico of 479 - 500 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 499 J/(kg·K) Show Material materials with Calor específico of 499 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 499 - 550 J/(kg·K) Show Material materials with Calor específico of 499 - 550 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 550 J/(kg·K) Show Material materials with Calor específico of 550 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 517 J/(kg·K) Show Material materials with Calor específico of 517 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 517 - 590 J/(kg·K) Show Material materials with Calor específico of 517 - 590 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 590 J/(kg·K) Show Material materials with Calor específico of 590 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
400 °C | 536 J/(kg·K) Show Material materials with Calor específico of 536 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
500 °C | 558 J/(kg·K) Show Material materials with Calor específico of 558 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
600 °C | 587 J/(kg·K) Show Material materials with Calor específico of 587 J/(kg·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
Coeficiente de dilatación térmica | -100 °C | 1.08e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.08e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
20 °C | 1.19e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.19e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 1.11e-05 - 1.25e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.11e-05 - 1.25e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 1.11e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.11e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 1.25e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.25e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 1.21e-05 - 1.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.21e-05 - 1.3e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 1.21e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.21e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 1.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 1.29e-05 - 1.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29e-05 - 1.36e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 1.29e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 1.36e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.36e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
400 °C | 1.35e-05 - 1.41e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35e-05 - 1.41e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
400 °C | 1.35e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
400 °C | 1.41e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.41e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
500 °C | 1.45e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.45e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
600 °C | 1.49e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.49e-05 1/K | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
Conductividad térmica | 20 °C | 41.7 W/(m·K) Show Material materials with Conductividad térmica of 41.7 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
20 °C | 41.7 - 52 W/(m·K) Show Material materials with Conductividad térmica of 41.7 - 52 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
20 °C | 52 W/(m·K) Show Material materials with Conductividad térmica of 52 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 43.4 W/(m·K) Show Material materials with Conductividad térmica of 43.4 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 43.4 - 50.6 W/(m·K) Show Material materials with Conductividad térmica of 43.4 - 50.6 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
100 °C | 50.6 W/(m·K) Show Material materials with Conductividad térmica of 50.6 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 43.2 W/(m·K) Show Material materials with Conductividad térmica of 43.2 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 43.2 - 48.1 W/(m·K) Show Material materials with Conductividad térmica of 43.2 - 48.1 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 48.1 W/(m·K) Show Material materials with Conductividad térmica of 48.1 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 41.4 W/(m·K) Show Material materials with Conductividad térmica of 41.4 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 41.4 - 45.7 W/(m·K) Show Material materials with Conductividad térmica of 41.4 - 45.7 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 45.7 W/(m·K) Show Material materials with Conductividad térmica of 45.7 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
400 °C | 39.1 W/(m·K) Show Material materials with Conductividad térmica of 39.1 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
500 °C | 36.7 W/(m·K) Show Material materials with Conductividad térmica of 36.7 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
600 °C | 34.1 W/(m·K) Show Material materials with Conductividad térmica of 34.1 W/(m·K) | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
Difusividad térmica | 20 °C | 11.6 mm²/s Show Material materials with Difusividad térmica of 11.6 mm²/s | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
100 °C | 11.3 mm²/s Show Material materials with Difusividad térmica of 11.3 mm²/s | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
200 °C | 10.5 mm²/s Show Material materials with Difusividad térmica of 10.5 mm²/s | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
300 °C | 9.5 mm²/s Show Material materials with Difusividad térmica of 9.5 mm²/s | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
400 °C | 8.3 mm²/s Show Material materials with Difusividad térmica of 8.3 mm²/s | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
500 °C | 7.1 mm²/s Show Material materials with Difusividad térmica of 7.1 mm²/s | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
600 °C | 5.8 mm²/s Show Material materials with Difusividad térmica of 5.8 mm²/s | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | ||
Temperatura de fusión | 1380 - 1514 °C Show Material materials with Temperatura de fusión of 1380 - 1514 °C | Typical for Medium Carbon Steel | ||||
Temperatura máx. de funcionamiento | -25 - 480 °C Show Material materials with Temperatura máx. de funcionamiento of -25 - 480 °C | soft annealed (+A) | EN 10083-1, EN 10083-2, EN 10083-3 | Strip, Sheet, Flat, Bar, Wire, Forging | Long | |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Resistividad eléctrica | 20 °C | 1.2e-07 - 2.5e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.2e-07 - 2.5e-07 Ω·m | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
20 °C | 1.2e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.2e-07 Ω·m | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
20 °C | 2.5e-07 Ω·m Show Material materials with Resistividad eléctrica of 2.5e-07 Ω·m | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
100 °C | 2.95e-07 Ω·m Show Material materials with Resistividad eléctrica of 2.95e-07 Ω·m | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
200 °C | 3.65e-07 Ω·m Show Material materials with Resistividad eléctrica of 3.65e-07 Ω·m | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
300 °C | 4.53e-07 Ω·m Show Material materials with Resistividad eléctrica of 4.53e-07 Ω·m | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
400 °C | 5.56e-07 Ω·m Show Material materials with Resistividad eléctrica of 5.56e-07 Ω·m | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
500 °C | 6.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 6.74e-07 Ω·m | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
600 °C | 8.13e-07 Ω·m Show Material materials with Resistividad eléctrica of 8.13e-07 Ω·m | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1, EN 10083-3 | Bar, wire, Flat, Sheet, Strip, Forging, Wire |
Carbono | 0.42 - 0.5 % Show Material materials with Carbono of 0.42 - 0.5 % | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1, EN 10083-3 | Bar, wire, Flat, Sheet, Strip, Forging, Wire |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
Cromo | 0.4 % Show Material materials with Cromo of 0.4 % | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
0.03 % Show Material materials with Fósforo of 0.03 % | soft annealed (+A) | EN 10083-1, EN 10083-2, ISO 683-1 | Bar, wire, Flat, Sheet, Strip, Forging | |
0.035 % Show Material materials with Fósforo of 0.035 % | soft annealed (+A) | EN 10083-1, EN 10083-2, EN 10083-3, ISO 683-1 | Strip, Sheet, Flat, Bar, Wire, Forging | |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1, EN 10083-3 | Bar, wire, Flat, Sheet, Strip, Forging, Wire |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
Silicona | 0.1 - 0.4 % Show Material materials with Silicona of 0.1 - 0.4 % | soft annealed (+A) | ISO 683-1, EN 10083-2, EN 10083-1 | Bar, wire, Flat, Sheet, Strip, Forging |
0.4 % Show Material materials with Silicona of 0.4 % | soft annealed (+A) | EN 10083-1, EN 10083-2, ISO 683-1, EN 10083-3 | Bar, wire, Flat, Sheet, Strip, Forging, Wire |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |