General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 22 % Show Material materials with Elongación of 22 % | |
Elongación transversal | 20.0 °C | 20 % Show Material materials with Elongación transversal of 20 % | |
Límite elástico Rp0.5 | 20.0 °C | 360 - 510 MPa Show Material materials with Límite elástico Rp0.5 of 360 - 510 MPa | |
Límite elástico transversal | 20.0 °C | 360 - 510 MPa Show Material materials with Límite elástico transversal of 360 - 510 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 460 MPa Show Material materials with Resistencia a la tracción of 460 MPa | |
Resistencia a la tracción transversal | 20.0 °C | 460 MPa Show Material materials with Resistencia a la tracción transversal of 460 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.015 - 0.06 % Show Material materials with Aluminio of 0.015 - 0.06 % |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.16 % Show Material materials with Carbono of 0.16 % |
Cobre | 0.25 % Show Material materials with Cobre of 0.25 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1.4 % Show Material materials with Manganeso of 1.4 % |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Silicona | 0.45 % Show Material materials with Silicona of 0.45 % |
Titanio | 0.04 % Show Material materials with Titanio of 0.04 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |