General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8 g/cm³ Show Material materials with Densidad of 8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Elongación A80 transversal | 20.0 °C | 35 - 40 % Show Material materials with Elongación A80 transversal of 35 - 40 % | |
Elongación transversal | 20.0 °C | 35 - 40 % Show Material materials with Elongación transversal of 35 - 40 % | |
Límite elástico Rp 0,2 | 50.0 °C | 248 MPa Show Material materials with Límite elástico Rp 0,2 of 248 MPa | |
100.0 °C | 211 MPa Show Material materials with Límite elástico Rp 0,2 of 211 MPa | ||
150.0 °C | 185 MPa Show Material materials with Límite elástico Rp 0,2 of 185 MPa | ||
200.0 °C | 167 MPa Show Material materials with Límite elástico Rp 0,2 of 167 MPa | ||
250.0 °C | 155 MPa Show Material materials with Límite elástico Rp 0,2 of 155 MPa | ||
300.0 °C | 145 MPa Show Material materials with Límite elástico Rp 0,2 of 145 MPa | ||
350.0 °C | 140 MPa Show Material materials with Límite elástico Rp 0,2 of 140 MPa | ||
400.0 °C | 135 MPa Show Material materials with Límite elástico Rp 0,2 of 135 MPa | ||
450.0 °C | 131 MPa Show Material materials with Límite elástico Rp 0,2 of 131 MPa | ||
500.0 °C | 129 MPa Show Material materials with Límite elástico Rp 0,2 of 129 MPa | ||
550.0 °C | 127 MPa Show Material materials with Límite elástico Rp 0,2 of 127 MPa | ||
Límite elástico Rp 1,0 | 50.0 °C | 286 MPa Show Material materials with Límite elástico Rp 1,0 of 286 MPa | |
100.0 °C | 246 MPa Show Material materials with Límite elástico Rp 1,0 of 246 MPa | ||
150.0 °C | 218 MPa Show Material materials with Límite elástico Rp 1,0 of 218 MPa | ||
200.0 °C | 198 MPa Show Material materials with Límite elástico Rp 1,0 of 198 MPa | ||
250.0 °C | 183 MPa Show Material materials with Límite elástico Rp 1,0 of 183 MPa | ||
300.0 °C | 175 MPa Show Material materials with Límite elástico Rp 1,0 of 175 MPa | ||
350.0 °C | 169 MPa Show Material materials with Límite elástico Rp 1,0 of 169 MPa | ||
400.0 °C | 164 MPa Show Material materials with Límite elástico Rp 1,0 of 164 MPa | ||
450.0 °C | 160 MPa Show Material materials with Límite elástico Rp 1,0 of 160 MPa | ||
500.0 °C | 158 MPa Show Material materials with Límite elástico Rp 1,0 of 158 MPa | ||
550.0 °C | 157 MPa Show Material materials with Límite elástico Rp 1,0 of 157 MPa | ||
Límite elástico transversal Rp 0,2 | 20.0 °C | 270 - 290 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 270 - 290 MPa | |
Límite elástico transversal Rp 1,0 | 20.0 °C | 310 - 320 MPa Show Material materials with Límite elástico transversal Rp 1,0 of 310 - 320 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 20.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | |
100.0 °C | 194 GPa Show Material materials with Módulo elástico of 194 GPa | ||
200.0 °C | 186 GPa Show Material materials with Módulo elástico of 186 GPa | ||
300.0 °C | 179 GPa Show Material materials with Módulo elástico of 179 GPa | ||
400.0 °C | 172 GPa Show Material materials with Módulo elástico of 172 GPa | ||
500.0 °C | 165 GPa Show Material materials with Módulo elástico of 165 GPa | ||
Resistencia a la tracción | 20.0 °C | 540 - 770 MPa Show Material materials with Resistencia a la tracción of 540 - 770 MPa | |
50.0 °C | 525 MPa Show Material materials with Resistencia a la tracción of 525 MPa | ||
100.0 °C | 500 MPa Show Material materials with Resistencia a la tracción of 500 MPa | ||
150.0 °C | 470 MPa Show Material materials with Resistencia a la tracción of 470 MPa | ||
200.0 °C | 440 MPa Show Material materials with Resistencia a la tracción of 440 MPa | ||
250.0 °C | 430 MPa Show Material materials with Resistencia a la tracción of 430 MPa | ||
300.0 °C | 420 MPa Show Material materials with Resistencia a la tracción of 420 MPa | ||
350.0 °C | 415 MPa Show Material materials with Resistencia a la tracción of 415 MPa | ||
400.0 °C | 415 MPa Show Material materials with Resistencia a la tracción of 415 MPa | ||
450.0 °C | 415 MPa Show Material materials with Resistencia a la tracción of 415 MPa | ||
500.0 °C | 410 MPa Show Material materials with Resistencia a la tracción of 410 MPa | ||
550.0 °C | 390 MPa Show Material materials with Resistencia a la tracción of 390 MPa | ||
Resistencia a la tracción transversal | 20.0 °C | 540 - 770 MPa Show Material materials with Resistencia a la tracción transversal of 540 - 770 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | |
200.0 °C | 1.65E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.65E-5 1/K | ||
300.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | ||
400.0 °C | 1.75E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K | ||
500.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | ||
Conductividad térmica | 20.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) | |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 7.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 7.5E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cromo | 16.5 - 19.5 % Show Material materials with Cromo of 16.5 - 19.5 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 3 - 4 % Show Material materials with Molibdeno of 3 - 4 % |
Nitrógeno | 0.1 - 0.2 % Show Material materials with Nitrógeno of 0.1 - 0.2 % |
Níquel | 10.5 - 14 % Show Material materials with Níquel of 10.5 - 14 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |