General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 6 % Show Material materials with Elongación of 6 % | |
Estricción | 20.0 °C | 35 % Show Material materials with Estricción of 35 % | |
Límite elástico Rp 0,2 | 20.0 °C | 1400 MPa Show Material materials with Límite elástico Rp 0,2 of 1400 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 1550 - 1850 MPa Show Material materials with Resistencia a la tracción of 1550 - 1850 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.42 - 0.5 % Show Material materials with Carbono of 0.42 - 0.5 % |
Cromo | 0.5 - 0.8 % Show Material materials with Cromo of 0.5 - 0.8 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Molibdeno | 0.2 - 0.3 % Show Material materials with Molibdeno of 0.2 - 0.3 % |
Silicona | 1.3 - 1.7 % Show Material materials with Silicona of 1.3 - 1.7 % |
Technological properties
Property | ||
---|---|---|
Features | Spring |