General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Elongación | 20.0 °C | 6 % Show Material materials with Elongación of 6 % | |
Estricción | 20.0 °C | 30 % Show Material materials with Estricción of 30 % | |
Límite elástico Rp 0,2 | 20.0 °C | 1300 MPa Show Material materials with Límite elástico Rp 0,2 of 1300 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 1450 - 1750 MPa Show Material materials with Resistencia a la tracción of 1450 - 1750 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Calor específico of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Conductividad térmica | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.56 - 0.64 % Show Material materials with Carbono of 0.56 - 0.64 % |
Cromo | 0.7 - 1 % Show Material materials with Cromo of 0.7 - 1 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.7 - 1 % Show Material materials with Manganeso of 0.7 - 1 % |
Molibdeno | 0.06 - 0.15 % Show Material materials with Molibdeno of 0.06 - 0.15 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |
Technological properties
Property | ||
---|---|---|
Features | Spring |