General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Elongación | 20.0 °C | 16 % Show Material materials with Elongación of 16 % | |
Límite elástico Rp 0,2 | 20.0 °C | 420 MPa Show Material materials with Límite elástico Rp 0,2 of 420 MPa | |
200.0 °C | 390 MPa Show Material materials with Límite elástico Rp 0,2 of 390 MPa | ||
300.0 °C | 380 MPa Show Material materials with Límite elástico Rp 0,2 of 380 MPa | ||
400.0 °C | 370 MPa Show Material materials with Límite elástico Rp 0,2 of 370 MPa | ||
500.0 °C | 305 MPa Show Material materials with Límite elástico Rp 0,2 of 305 MPa | ||
550.0 °C | 250 MPa Show Material materials with Límite elástico Rp 0,2 of 250 MPa | ||
Límite elástico Rp 1,0 | 20.0 °C | 210 MPa Show Material materials with Límite elástico Rp 1,0 of 210 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 630 - 760 MPa Show Material materials with Resistencia a la tracción of 630 - 760 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.18E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.18E-5 1/K | |
300.0 °C | 1.23E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.23E-5 1/K | ||
500.0 °C | 1.27E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.27E-5 1/K | ||
Conductividad térmica | 50.0 °C | 30.1 W/(m·K) Show Material materials with Conductividad térmica of 30.1 W/(m·K) | |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.12 - 0.19 % Show Material materials with Carbono of 0.12 - 0.19 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 4 - 6 % Show Material materials with Cromo of 4 - 6 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Molibdeno | 0.45 - 0.65 % Show Material materials with Molibdeno of 0.45 - 0.65 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |