General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Elongación | 20.0 °C | 17 % Show Material materials with Elongación of 17 % | |
Límite elástico Rp 0,2 | 20.0 °C | 295 MPa Show Material materials with Límite elástico Rp 0,2 of 295 MPa | |
100.0 °C | 264 MPa Show Material materials with Límite elástico Rp 0,2 of 264 MPa | ||
200.0 °C | 244 MPa Show Material materials with Límite elástico Rp 0,2 of 244 MPa | ||
300.0 °C | 230 MPa Show Material materials with Límite elástico Rp 0,2 of 230 MPa | ||
400.0 °C | 214 MPa Show Material materials with Límite elástico Rp 0,2 of 214 MPa | ||
500.0 °C | 194 MPa Show Material materials with Límite elástico Rp 0,2 of 194 MPa | ||
550.0 °C | 144 MPa Show Material materials with Límite elástico Rp 0,2 of 144 MPa | ||
Límite elástico Rp 1,0 | 20.0 °C | 200 MPa Show Material materials with Límite elástico Rp 1,0 of 200 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 510 - 660 MPa Show Material materials with Resistencia a la tracción of 510 - 660 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Conductividad térmica | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.1 - 0.15 % Show Material materials with Carbono of 0.1 - 0.15 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 0.3 - 0.5 % Show Material materials with Cromo of 0.3 - 0.5 % |
Estaño | 0.03 % Show Material materials with Estaño of 0.03 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 0.7 % Show Material materials with Manganeso of 0.4 - 0.7 % |
Molibdeno | 0.4 - 0.6 % Show Material materials with Molibdeno of 0.4 - 0.6 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 0.45 % Show Material materials with Silicona of 0.45 % |
Vanadio | 0.22 - 0.3 % Show Material materials with Vanadio of 0.22 - 0.3 % |