Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Molybdenum Steel |
Elongación | 20.0 °C | 23 % Show Material materials with Elongación of 23 % | |
Límite elástico Rp 0,2 | 20.0 °C | 240 MPa Show Material materials with Límite elástico Rp 0,2 of 240 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Molybdenum Steel |
Resistencia a la tracción | 20.0 °C | 440 - 790 MPa Show Material materials with Resistencia a la tracción of 440 - 790 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.24E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.24E-5 1/K | |
300.0 °C | 1.31E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.31E-5 1/K | ||
500.0 °C | 1.38E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.38E-5 1/K | ||
Conductividad térmica | 50.0 °C | 43 W/(m·K) Show Material materials with Conductividad térmica of 43 W/(m·K) | |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Molybdenum Steel | |
Temperatura máx. de funcionamiento, largo | -45 - 0 °C Show Material materials with Temperatura máx. de funcionamiento, largo of -45 - 0 °C |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.15 - 0.2 % Show Material materials with Carbono of 0.15 - 0.2 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.8 - 1.2 % Show Material materials with Manganeso of 0.8 - 1.2 % |
Molibdeno | 0.45 - 0.65 % Show Material materials with Molibdeno of 0.45 - 0.65 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |