Material GX3CrNi13-4 is equivalent to trademark G-X 3 CrNi 13 4 acc. to SEW 685-89. It combines high strength and very good cryogenic properties. It is used at low temperatures in refrigerator construction up to approx. -120 °C. Material G-X 5 CrNi 13 4, material number 1.4313 is acc. to VdTÜV-material specification 452 applicable for pressure vessels acc. to TRB 100 (and AD-data sheets W5 and W10) from -120 to 20 °C. Further application for blade and guide wheels for pumps, compressors and turbines as well as for pump casings and machine components in hydraulic installations from -120 to 20 °C. Further application in the nuclear power engineering if the relevant specifications allow the application at -120 to 20 °C. The welding suitability of the steel cast is examined for the welding methods TIG-welding, metal arc welding and submerged welding. After the welding the material have to cool down under 80 deg. for an following heat-treatment. An double tempering or stress relieve annealing is possible. After the double tempering an decrease of the strength should considered. The cooling rate until below 300 °C should not exceed 80 K/h. By the welding in the production of thin-walled parts its possible to abandon the pre-heating, tempering or stress relieve annealing if appropriate verification was done.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

7.7 g/cm³

Show Material materials with Densidad of 7.7 g/cm³

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

23.0 °C

0.3 [-]

Show Material materials with Coeficiente de Poisson of 0.3 [-]

Typical for Steel

Elongación

20.0 °C

15 %

Show Material materials with Elongación of 15 %

Límite elástico Rp 0,2

20.0 °C

500 MPa

Show Material materials with Límite elástico Rp 0,2 of 500 MPa

100.0 °C

515 MPa

Show Material materials with Límite elástico Rp 0,2 of 515 MPa

150.0 °C

500 MPa

Show Material materials with Límite elástico Rp 0,2 of 500 MPa

200.0 °C

485 MPa

Show Material materials with Límite elástico Rp 0,2 of 485 MPa

250.0 °C

470 MPa

Show Material materials with Límite elástico Rp 0,2 of 470 MPa

300.0 °C

455 MPa

Show Material materials with Límite elástico Rp 0,2 of 455 MPa

Módulo elástico

23.0 °C

190 - 210 GPa

Show Material materials with Módulo elástico of 190 - 210 GPa

Typical for Steel

Resistencia a la tracción

20.0 °C

700 - 900 MPa

Show Material materials with Resistencia a la tracción of 700 - 900 MPa

Aplicaciones térmicas

PropertyTemperatureValue

Calor específico

20.0 °C

460 J/(kg·K)

Show Material materials with Calor específico of 460 J/(kg·K)

Coeficiente de dilatación térmica

-195.0 °C

8.6E-6 1/K

Show Material materials with Coeficiente de dilatación térmica of 8.6E-6 1/K

-170.0 °C

9.3E-6 1/K

Show Material materials with Coeficiente de dilatación térmica of 9.3E-6 1/K

-120.0 °C

1.01E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.01E-5 1/K

-50.0 °C

1.08E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.08E-5 1/K

-25.0 °C

1.1E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 1/K

100.0 °C

1.05E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.05E-5 1/K

300.0 °C

1.1E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 1/K

500.0 °C

1.2E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K

Unlock all property charts

Conductividad térmica

-20.0 °C

30 W/(m·K)

Show Material materials with Conductividad térmica of 30 W/(m·K)

50.0 °C

26 W/(m·K)

Show Material materials with Conductividad térmica of 26 W/(m·K)

100.0 °C

27 W/(m·K)

Show Material materials with Conductividad térmica of 27 W/(m·K)

Unlock all property charts

Temperatura máx. de funcionamiento, largo

-120 - 20 °C

Show Material materials with Temperatura máx. de funcionamiento, largo of -120 - 20 °C

Chemical properties

PropertyValue

Azufre

0.015 %

Show Material materials with Azufre of 0.015 %

Carbono

0.05 %

Show Material materials with Carbono of 0.05 %

Cobre

0.3 %

Show Material materials with Cobre of 0.3 %

Cromo

12 - 13.5 %

Show Material materials with Cromo of 12 - 13.5 %

Fósforo

0.04 %

Show Material materials with Fósforo of 0.04 %

Manganeso

1 %

Show Material materials with Manganeso of 1 %

Molibdeno

0.7 %

Show Material materials with Molibdeno of 0.7 %

Níquel

3.5 - 5 %

Show Material materials with Níquel of 3.5 - 5 %

Silicona

1 %

Show Material materials with Silicona of 1 %

Vanadio

0.08 %

Show Material materials with Vanadio of 0.08 %