General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel |
Elongación | 20.0 °C | 21 - 24 % Show Material materials with Elongación of 21 - 24 % | |
Límite elástico | 20.0 °C | 265 - 285 MPa Show Material materials with Límite elástico of 265 - 285 MPa | |
200.0 °C | 206 MPa Show Material materials with Límite elástico of 206 MPa | ||
250.0 °C | 186 MPa Show Material materials with Límite elástico of 186 MPa | ||
300.0 °C | 157 MPa Show Material materials with Límite elástico of 157 MPa | ||
350.0 °C | 137 MPa Show Material materials with Límite elástico of 137 MPa | ||
400.0 °C | 118 MPa Show Material materials with Límite elástico of 118 MPa | ||
Límite elástico Rp 0,2 | 20.0 °C | 255 - 275 MPa Show Material materials with Límite elástico Rp 0,2 of 255 - 275 MPa | |
50.0 °C | 251 - 276 MPa Show Material materials with Límite elástico Rp 0,2 of 251 - 276 MPa | ||
100.0 °C | 237 - 259 MPa Show Material materials with Límite elástico Rp 0,2 of 237 - 259 MPa | ||
150.0 °C | 219 - 240 MPa Show Material materials with Límite elástico Rp 0,2 of 219 - 240 MPa | ||
200.0 °C | 201 - 221 MPa Show Material materials with Límite elástico Rp 0,2 of 201 - 221 MPa | ||
250.0 °C | 184 - 202 MPa Show Material materials with Límite elástico Rp 0,2 of 184 - 202 MPa | ||
300.0 °C | 151 - 166 MPa Show Material materials with Límite elástico Rp 0,2 of 151 - 166 MPa | ||
350.0 °C | 137 - 153 MPa Show Material materials with Límite elástico Rp 0,2 of 137 - 153 MPa | ||
400.0 °C | 118 - 144 MPa Show Material materials with Límite elástico Rp 0,2 of 118 - 144 MPa | ||
Módulo de cizallamiento | 23.0 °C | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel |
Resistencia a la tracción | 20.0 °C | 390 - 510 MPa Show Material materials with Resistencia a la tracción of 390 - 510 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 23.0 °C | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 - 0.06 % Show Material materials with Aluminio of 0.02 - 0.06 % |
Azufre | 0.01 - 0.015 % Show Material materials with Azufre of 0.01 - 0.015 % |
Carbono | 0.18 % Show Material materials with Carbono of 0.18 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.6 - 1.5 % Show Material materials with Manganeso of 0.6 - 1.5 % |
Molibdeno | 0.08 % Show Material materials with Molibdeno of 0.08 % |
Niobio | 0.03 % Show Material materials with Niobio of 0.03 % |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % |