General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 19 % Show Material materials with Elongación of 19 % | |
Límite elástico | 20.0 °C | 400 - 460 MPa Show Material materials with Límite elástico of 400 - 460 MPa | |
200.0 °C | 343 MPa Show Material materials with Límite elástico of 343 MPa | ||
250.0 °C | 314 MPa Show Material materials with Límite elástico of 314 MPa | ||
300.0 °C | 294 MPa Show Material materials with Límite elástico of 294 MPa | ||
350.0 °C | 265 MPa Show Material materials with Límite elástico of 265 MPa | ||
400.0 °C | 235 MPa Show Material materials with Límite elástico of 235 MPa | ||
Límite elástico Rp 0,2 | 50.0 °C | 385 - 445 MPa Show Material materials with Límite elástico Rp 0,2 of 385 - 445 MPa | |
100.0 °C | 353 - 425 MPa Show Material materials with Límite elástico Rp 0,2 of 353 - 425 MPa | ||
150.0 °C | 324 - 405 MPa Show Material materials with Límite elástico Rp 0,2 of 324 - 405 MPa | ||
200.0 °C | 304 - 380 MPa Show Material materials with Límite elástico Rp 0,2 of 304 - 380 MPa | ||
250.0 °C | 275 - 360 MPa Show Material materials with Límite elástico Rp 0,2 of 275 - 360 MPa | ||
300.0 °C | 255 - 340 MPa Show Material materials with Límite elástico Rp 0,2 of 255 - 340 MPa | ||
350.0 °C | 226 - 265 MPa Show Material materials with Límite elástico Rp 0,2 of 226 - 265 MPa | ||
400.0 °C | 196 - 235 MPa Show Material materials with Límite elástico Rp 0,2 of 196 - 235 MPa | ||
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 500 - 720 MPa Show Material materials with Resistencia a la tracción of 500 - 720 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.018 % Show Material materials with Aluminio of 0.018 % |
Azufre | 0.01 - 0.015 % Show Material materials with Azufre of 0.01 - 0.015 % |
Boro | 5E-3 % Show Material materials with Boro of 5E-3 % |
Carbono | 0.18 % Show Material materials with Carbono of 0.18 % |
Circonio | 0.05 % Show Material materials with Circonio of 0.05 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 0.5 % Show Material materials with Cromo of 0.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1.7 % Show Material materials with Manganeso of 1.7 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % |
Vanadio | 0.08 % Show Material materials with Vanadio of 0.08 % |