General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 14 % Show Material materials with Elongación of 14 % | |
Límite elástico | 20.0 °C | 630 - 690 MPa Show Material materials with Límite elástico of 630 - 690 MPa | |
Límite elástico Rp 0,2 | 50.0 °C | 610 - 670 MPa Show Material materials with Límite elástico Rp 0,2 of 610 - 670 MPa | |
100.0 °C | 585 - 645 MPa Show Material materials with Límite elástico Rp 0,2 of 585 - 645 MPa | ||
150.0 °C | 555 - 615 MPa Show Material materials with Límite elástico Rp 0,2 of 555 - 615 MPa | ||
200.0 °C | 535 - 595 MPa Show Material materials with Límite elástico Rp 0,2 of 535 - 595 MPa | ||
250.0 °C | 515 - 575 MPa Show Material materials with Límite elástico Rp 0,2 of 515 - 575 MPa | ||
300.0 °C | 510 - 570 MPa Show Material materials with Límite elástico Rp 0,2 of 510 - 570 MPa | ||
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 720 - 940 MPa Show Material materials with Resistencia a la tracción of 720 - 940 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.018 % Show Material materials with Aluminio of 0.018 % |
Azufre | 0.01 - 0.015 % Show Material materials with Azufre of 0.01 - 0.015 % |
Boro | 5E-3 % Show Material materials with Boro of 5E-3 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Circonio | 0.15 % Show Material materials with Circonio of 0.15 % |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % |
Cromo | 1.5 % Show Material materials with Cromo of 1.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1.7 % Show Material materials with Manganeso of 1.7 % |
Molibdeno | 0.7 % Show Material materials with Molibdeno of 0.7 % |
Niobio | 0.05 - 0.06 % Show Material materials with Niobio of 0.05 - 0.06 % |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % |
Níquel | 2.5 % Show Material materials with Níquel of 2.5 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % |
Vanadio | 0.12 % Show Material materials with Vanadio of 0.12 % |