General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.84 g/cm³ Show Material materials with Densidad of 7.84 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 11 % Show Material materials with Elongación of 11 % | |
Límite elástico | 20.0 °C | 830 - 890 MPa Show Material materials with Límite elástico of 830 - 890 MPa | |
Módulo elástico | 20.0 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | |
Resistencia a la tracción | 20.0 °C | 880 - 1100 MPa Show Material materials with Resistencia a la tracción of 880 - 1100 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 20.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) |
Coeficiente de dilatación térmica | 100.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K |
Conductividad térmica | 20.0 °C | 38 W/(m·K) Show Material materials with Conductividad térmica of 38 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 2.8E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.8E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Boro | 5E-3 % Show Material materials with Boro of 5E-3 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Circonio | 0.15 % Show Material materials with Circonio of 0.15 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 1.5 % Show Material materials with Cromo of 1.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 1.7 % Show Material materials with Manganeso of 1.7 % |
Molibdeno | 0.7 % Show Material materials with Molibdeno of 0.7 % |
Niobio | 0.06 % Show Material materials with Niobio of 0.06 % |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % |
Níquel | 2 % Show Material materials with Níquel of 2 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % |
Vanadio | 0.12 % Show Material materials with Vanadio of 0.12 % |