General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.7 g/cm³ Show Material materials with Densidad of 7.7 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Martensitic Stainless Steel |
Límite elástico Rp 0,2 | 50.0 °C | 730 MPa Show Material materials with Límite elástico Rp 0,2 of 730 MPa | |
100.0 °C | 680 MPa Show Material materials with Límite elástico Rp 0,2 of 680 MPa | ||
150.0 °C | 668 MPa Show Material materials with Límite elástico Rp 0,2 of 668 MPa | ||
200.0 °C | 655 MPa Show Material materials with Límite elástico Rp 0,2 of 655 MPa | ||
250.0 °C | 653 MPa Show Material materials with Límite elástico Rp 0,2 of 653 MPa | ||
300.0 °C | 650 MPa Show Material materials with Límite elástico Rp 0,2 of 650 MPa | ||
350.0 °C | 630 MPa Show Material materials with Límite elástico Rp 0,2 of 630 MPa | ||
400.0 °C | 610 MPa Show Material materials with Límite elástico Rp 0,2 of 610 MPa | ||
450.0 °C | 560 MPa Show Material materials with Límite elástico Rp 0,2 of 560 MPa | ||
500.0 °C | 505 MPa Show Material materials with Límite elástico Rp 0,2 of 505 MPa | ||
550.0 °C | 400 MPa Show Material materials with Límite elástico Rp 0,2 of 400 MPa | ||
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Martensitic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Martensitic Stainless Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Conductividad térmica | 23.0 °C | 14 - 31 W/(m·K) Show Material materials with Conductividad térmica of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Temperatura de fusión | 1370 - 1530 °C Show Material materials with Temperatura de fusión of 1370 - 1530 °C | Typical for Martensitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.08 - 0.15 % Show Material materials with Carbono of 0.08 - 0.15 % |
Cromo | 11 - 12.5 % Show Material materials with Cromo of 11 - 12.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 0.9 % Show Material materials with Manganeso of 0.4 - 0.9 % |
Molibdeno | 1.5 - 2 % Show Material materials with Molibdeno of 1.5 - 2 % |
Nitrógeno | 0.02 - 0.04 % Show Material materials with Nitrógeno of 0.02 - 0.04 % |
Níquel | 2 - 3 % Show Material materials with Níquel of 2 - 3 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Vanadio | 0.25 - 0.4 % Show Material materials with Vanadio of 0.25 - 0.4 % |