General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | ||||
Dureza Brinell | 253 [-] Show Material materials with Dureza Brinell of 253 [-] | Predicted Value, Transverse | ||||
Elongación | 18.1 % Show Material materials with Elongación of 18.1 % | Predicted Value, A200 | ||||
19.7 % Show Material materials with Elongación of 19.7 % | Predicted Value, A80 Transverse | |||||
20.7 % Show Material materials with Elongación of 20.7 % | Predicted Value, A5 | |||||
23.6 % Show Material materials with Elongación of 23.6 % | Predicted Value, Transverse | |||||
25.3 % Show Material materials with Elongación of 25.3 % | Predicted Value, A50 | |||||
20 °C | 24 % Show Material materials with Elongación of 24 % | normalized or normalized formed (+N) | EN 10120 | Flat | A80 | |
20 °C | 32 % Show Material materials with Elongación of 32 % | normalized or normalized formed (+N) | EN 10120 | Flat | ||
Estricción | 42.0 % Show Material materials with Estricción of 42.0 % | Predicted Value, Transverse | ||||
44.5 % Show Material materials with Estricción of 44.5 % | Predicted Value | |||||
Límite elástico | 258.2 MPa Show Material materials with Límite elástico of 258.2 MPa | Predicted Value, RP1 | ||||
310.3 MPa Show Material materials with Límite elástico of 310.3 MPa | Predicted Value, Transverse | |||||
328.5 MPa Show Material materials with Límite elástico of 328.5 MPa | Predicted Value, RP1 Transverse | |||||
362.6 MPa Show Material materials with Límite elástico of 362.6 MPa | Predicted Value, RP05 | |||||
447.9 MPa Show Material materials with Límite elástico of 447.9 MPa | Predicted Value, RP002 | |||||
464.2 MPa Show Material materials with Límite elástico of 464.2 MPa | Predicted Value, RP02 Transverse | |||||
20 °C | 265 MPa Show Material materials with Límite elástico of 265 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | ||
100 °C | 235 MPa Show Material materials with Límite elástico of 235 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
150 °C | 215 MPa Show Material materials with Límite elástico of 215 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
200 °C | 185 MPa Show Material materials with Límite elástico of 185 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
250 °C | 165 MPa Show Material materials with Límite elástico of 165 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
300 °C | 135 MPa Show Material materials with Límite elástico of 135 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | RP02 | |
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | ||||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Resistencia a la tracción | 20 °C | 410 - 500 MPa Show Material materials with Resistencia a la tracción of 410 - 500 MPa | normalized or normalized formed (+N) | EN 10120 | Flat | |
Resistencia al cizallamiento | 515.6 MPa Show Material materials with Resistencia al cizallamiento of 515.6 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 289.4 °C Show Material materials with Temperatura máx. de funcionamiento of 289.4 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 7 S/m Show Material materials with Conductividad eléctrica of 7 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Carbono | 0.19 % Show Material materials with Carbono of 0.19 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Manganeso | 0.4 % Show Material materials with Manganeso of 0.4 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Nitrógeno | 0.009 % Show Material materials with Nitrógeno of 0.009 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % | normalized or normalized formed (+N) | EN 10120 | Flat |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % | normalized or normalized formed (+N) | EN 10120 | Flat |