Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Elongación | 17.4 % Show Material materials with Elongación of 17.4 % | Predicted Value, A200 | ||||
17.7 % Show Material materials with Elongación of 17.7 % | Predicted Value, A80 | |||||
19.2 % Show Material materials with Elongación of 19.2 % | Predicted Value, A80 Transverse | |||||
20.5 % Show Material materials with Elongación of 20.5 % | Predicted Value, A5 | |||||
21.5 % Show Material materials with Elongación of 21.5 % | Predicted Value, Transverse | |||||
24.6 % Show Material materials with Elongación of 24.6 % | Predicted Value, A50 | |||||
20 °C | 22 % Show Material materials with Elongación of 22 % | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Estricción | 43.2 % Show Material materials with Estricción of 43.2 % | Predicted Value | ||||
43.3 % Show Material materials with Estricción of 43.3 % | Predicted Value, Transverse | |||||
Límite elástico | 263.3 MPa Show Material materials with Límite elástico of 263.3 MPa | Predicted Value, RP1 | ||||
323.3 MPa Show Material materials with Límite elástico of 323.3 MPa | Predicted Value, RP1 Transverse | |||||
370.4 MPa Show Material materials with Límite elástico of 370.4 MPa | Predicted Value, RP02 | |||||
375.5 MPa Show Material materials with Límite elástico of 375.5 MPa | Predicted Value, Transverse | |||||
429.9 MPa Show Material materials with Límite elástico of 429.9 MPa | Predicted Value, RP05 | |||||
471.8 MPa Show Material materials with Límite elástico of 471.8 MPa | Predicted Value, RP02 Transverse | |||||
498.9 MPa Show Material materials with Límite elástico of 498.9 MPa | Predicted Value, RP002 | |||||
20 °C | 315 MPa Show Material materials with Límite elástico of 315 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 335 MPa Show Material materials with Límite elástico of 335 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 355 MPa Show Material materials with Límite elástico of 355 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Módulo de cizallamiento | 80.1 GPa Show Material materials with Módulo de cizallamiento of 80.1 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 450 - 630 MPa Show Material materials with Resistencia a la tracción of 450 - 630 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | |
20 °C | 450 - 590 MPa Show Material materials with Resistencia a la tracción of 450 - 590 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 490 - 630 MPa Show Material materials with Resistencia a la tracción of 490 - 630 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 490 - 590 MPa Show Material materials with Resistencia a la tracción of 490 - 590 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Resistencia al cizallamiento | 543.6 MPa Show Material materials with Resistencia al cizallamiento of 543.6 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 449.7 J/(kg·K) Show Material materials with Calor específico of 449.7 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 12.02 1/K Show Material materials with Coeficiente de dilatación térmica of 12.02 1/K | Predicted Value |
Conductividad térmica | 37.01 W/(m·K) Show Material materials with Conductividad térmica of 37.01 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.008 % Show Material materials with Azufre of 0.008 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
0.01 % Show Material materials with Azufre of 0.01 % | quenched and tempered (+QT) | EN 10028-6 | Flat | |
Boro | 0.005 % Show Material materials with Boro of 0.005 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Carbono | 0.16 % Show Material materials with Carbono of 0.16 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Circonio | 0.05 % Show Material materials with Circonio of 0.05 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Molibdeno | 0.25 % Show Material materials with Molibdeno of 0.25 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Nitrógeno | 0.015 % Show Material materials with Nitrógeno of 0.015 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Vanadio | 0.06 % Show Material materials with Vanadio of 0.06 % | quenched and tempered (+QT) | EN 10028-6 | Flat |