General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.15 g/cm³ Show Material materials with Densidad of 7.15 g/cm³ | Typical for Grey Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.21 [-] Show Material materials with Coeficiente de Poisson of 0.21 [-] | Typical for Grey Cast Iron |
Dureza Brinell | 20.0 °C | 105 - 175 [-] Show Material materials with Dureza Brinell of 105 - 175 [-] | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 23.0 °C | 92.4 GPa Show Material materials with Módulo elástico of 92.4 GPa | Typical for Grey Cast Iron |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for Grey Cast Iron |
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.5E-5 1/K | Typical for Grey Cast Iron |
Conductividad térmica | 23.0 °C | 20 - 80 W/(m·K) Show Material materials with Conductividad térmica of 20 - 80 W/(m·K) | Typical for Grey Cast Iron |
Temperatura de fusión | 1127 - 1204 °C Show Material materials with Temperatura de fusión of 1127 - 1204 °C | Typical for Grey Cast Iron |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting |