General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.2 - 7.5 g/cm³ Show Material materials with Densidad of 7.2 - 7.5 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | Typical for Cast Iron |
Dureza Brinell | 20.0 °C | 150 [-] Show Material materials with Dureza Brinell of 150 [-] | |
Límite elástico Rp 0,2 | 20.0 °C | 200 MPa Show Material materials with Límite elástico Rp 0,2 of 200 MPa | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 20.0 °C | 175 - 195 GPa Show Material materials with Módulo elástico of 175 - 195 GPa | |
Resistencia a la tracción | 20.0 °C | 350 MPa Show Material materials with Resistencia a la tracción of 350 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 460 - 500 J/(kg·K) Show Material materials with Calor específico of 460 - 500 J/(kg·K) | |
Conductividad térmica | 20.0 °C | 50 - 63 W/(m·K) Show Material materials with Conductividad térmica of 50 - 63 W/(m·K) | |
Temperatura de fusión | 1120 °C Show Material materials with Temperatura de fusión of 1120 °C | Typical for Cast Iron |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 3E-7 - 4E-7 Ω·m Show Material materials with Resistividad eléctrica of 3E-7 - 4E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 0.1 - 0.15 % Show Material materials with Azufre of 0.1 - 0.15 % |
Carbono | 2.3 - 2.6 % Show Material materials with Carbono of 2.3 - 2.6 % |
Manganeso | 0.4 - 0.5 % Show Material materials with Manganeso of 0.4 - 0.5 % |
Silicona | 1.2 - 1.5 % Show Material materials with Silicona of 1.2 - 1.5 % |