General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Densidad of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | Typical for Cast Iron |
Dureza Brinell | 20.0 °C | 195 - 245 [-] Show Material materials with Dureza Brinell of 195 - 245 [-] | |
Límite elástico Rp 0,2 | 20.0 °C | 390 MPa Show Material materials with Límite elástico Rp 0,2 of 390 MPa | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 23.0 °C | 152 GPa Show Material materials with Módulo elástico of 152 GPa | Typical for Cast Iron |
Resistencia a la tracción | 20.0 °C | 600 MPa Show Material materials with Resistencia a la tracción of 600 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Calor específico of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Conductividad térmica | 23.0 °C | 55 W/(m·K) Show Material materials with Conductividad térmica of 55 W/(m·K) | Typical for Cast Iron |
Temperatura de fusión | 1120 °C Show Material materials with Temperatura de fusión of 1120 °C | Typical for Cast Iron |