Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A5 | 20.0 °C | 17 % Show Material materials with Elongación A5 of 17 % |
Límite elástico Rp 0,2 | 20.0 °C | 380 - 460 MPa Show Material materials with Límite elástico Rp 0,2 of 380 - 460 MPa |
Resistencia a la tracción | 20.0 °C | 510 - 720 MPa Show Material materials with Resistencia a la tracción of 510 - 720 MPa |
Resistencia al choque, ensayo Charpy entallado | -20.0 °C | 39 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 39 kJ/m² |
impactTransVNotch | -20.0 °C | 21 kJ/m² Show Material materials with impactTransVNotch of 21 kJ/m² |
Chemical properties
Property | Value |
---|---|
Aluminio | 0 - 0.02 % Show Material materials with Aluminio of 0 - 0.02 % |
Azufre | 0.03 - 0.035 % Show Material materials with Azufre of 0.03 - 0.035 % |
Boro | 0 - 5E-3 % Show Material materials with Boro of 0 - 5E-3 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Circonio | 0 - 0.15 % Show Material materials with Circonio of 0 - 0.15 % |
Cobre | 0.7 - 1.5 % Show Material materials with Cobre of 0.7 - 1.5 % |
Cromo | 0.7 - 2 % Show Material materials with Cromo of 0.7 - 2 % |
Fósforo | 0.03 - 0.04 % Show Material materials with Fósforo of 0.03 - 0.04 % |
Hierro | 90.44 - 99.3 % Show Material materials with Hierro of 90.44 - 99.3 % |
Manganeso | 0.7 - 1.7 % Show Material materials with Manganeso of 0.7 - 1.7 % |
Molibdeno | 0.4 - 1 % Show Material materials with Molibdeno of 0.4 - 1 % |
Niobio | 0 - 0.06 % Show Material materials with Niobio of 0 - 0.06 % |
Nitrógeno | 0 - 0.02 % Show Material materials with Nitrógeno of 0 - 0.02 % |
Níquel | 1 - 2 % Show Material materials with Níquel of 1 - 2 % |
Silicona | 0.5 - 0.55 % Show Material materials with Silicona of 0.5 - 0.55 % |
Titanio | 0 - 0.2 % Show Material materials with Titanio of 0 - 0.2 % |
Vanadio | 0 - 0.2 % Show Material materials with Vanadio of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Processing history | normalized, controlled rolled |