General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel |
Elongación A5 | 20.0 °C | 17 % Show Material materials with Elongación A5 of 17 % | |
Límite elástico Rp 0,2 | 20.0 °C | 380 - 460 MPa Show Material materials with Límite elástico Rp 0,2 of 380 - 460 MPa | |
Módulo de cizallamiento | 20.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel |
Resistencia a la tracción | 20.0 °C | 510 - 720 MPa Show Material materials with Resistencia a la tracción of 510 - 720 MPa | |
Resistencia al choque, ensayo Charpy entallado | -50.0 °C | 27 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 27 kJ/m² | |
impactTransVNotch | -50.0 °C | 16 kJ/m² Show Material materials with impactTransVNotch of 16 kJ/m² |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Temperatura de Curie | 20.0 °C | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0 - 0.02 % Show Material materials with Aluminio of 0 - 0.02 % |
Azufre | 0.025 - 0.03 % Show Material materials with Azufre of 0.025 - 0.03 % |
Boro | 0 - 5E-3 % Show Material materials with Boro of 0 - 5E-3 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Circonio | 0 - 0.15 % Show Material materials with Circonio of 0 - 0.15 % |
Cobre | 0.7 - 1.5 % Show Material materials with Cobre of 0.7 - 1.5 % |
Cromo | 0.7 - 2 % Show Material materials with Cromo of 0.7 - 2 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 90.45 - 99.3 % Show Material materials with Hierro of 90.45 - 99.3 % |
Manganeso | 0.7 - 1.7 % Show Material materials with Manganeso of 0.7 - 1.7 % |
Molibdeno | 0.4 - 1 % Show Material materials with Molibdeno of 0.4 - 1 % |
Niobio | 0 - 0.06 % Show Material materials with Niobio of 0 - 0.06 % |
Nitrógeno | 0 - 0.02 % Show Material materials with Nitrógeno of 0 - 0.02 % |
Níquel | 1 - 2 % Show Material materials with Níquel of 1 - 2 % |
Silicona | 0.5 - 0.55 % Show Material materials with Silicona of 0.5 - 0.55 % |
Titanio | 0 - 0.2 % Show Material materials with Titanio of 0 - 0.2 % |
Vanadio | 0 - 0.2 % Show Material materials with Vanadio of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Processing history | normalized, controlled rolled |