General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Molybdenum Steel |
Elongación A5 | 23.0 °C | 16 % Show Material materials with Elongación A5 of 16 % | |
Límite elástico | 23.0 °C | 480 MPa Show Material materials with Límite elástico of 480 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Molybdenum Steel |
Resistencia a la tracción | 23.0 °C | 620 - 790 MPa Show Material materials with Resistencia a la tracción of 620 - 790 MPa | |
Resistencia al choque, ensayo Charpy entallado | 20.0 °C | 40 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 40 kJ/m² |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.29E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29E-5 1/K | Typical for Molybdenum Steel |
Conductividad térmica | 23.0 °C | 37 - 48 W/(m·K) Show Material materials with Conductividad térmica of 37 - 48 W/(m·K) | Typical for Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Molybdenum Steel |