General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Medidas
Property | Value |
---|---|
Wall thickness | 1 - 8 mm Show Material materials with Wall thickness of 1 - 8 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Rockwell B | 23.0 °C | 90 [-] Show Material materials with Dureza Rockwell B of 90 [-] | |
Elongación A5 | 23.0 °C | 11 - 20 % Show Material materials with Elongación A5 of 11 - 20 % | |
Límite elástico Rp 0,2 | 23.0 °C | 205 MPa Show Material materials with Límite elástico Rp 0,2 of 205 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 390 MPa Show Material materials with Resistencia a la tracción of 390 MPa |