Property | Temperature | Value |
---|---|---|
Elongación A5 | 20.0 °C | 30 % Show Material materials with Elongación A5 of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 205 - 245 MPa Show Material materials with Límite elástico Rp 0,2 of 205 - 245 MPa |
Resistencia a la tracción | 20.0 °C | 550 MPa Show Material materials with Resistencia a la tracción of 550 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 14 - 17 % Show Material materials with Cromo of 14 - 17 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 6 - 10 % Show Material materials with Hierro of 6 - 10 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 72 % Show Material materials with Níquel of 72 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Technological properties
Property | ||
---|---|---|
Processing history | cold-finished, annealed |