Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A5 | 20.0 °C | 30 % Show Material materials with Elongación A5 of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 410 MPa Show Material materials with Límite elástico Rp 0,2 of 410 MPa |
Resistencia a la tracción | 20.0 °C | 820 MPa Show Material materials with Resistencia a la tracción of 820 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.4 % Show Material materials with Aluminio of 0.4 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cromo | 20 - 23 % Show Material materials with Cromo of 20 - 23 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 5 % Show Material materials with Hierro of 5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Molibdeno | 8 - 10 % Show Material materials with Molibdeno of 8 - 10 % |
Níquel | 58 % Show Material materials with Níquel of 58 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.4 % Show Material materials with Titanio of 0.4 % |
Technological properties
Property | ||
---|---|---|
Processing history | cold-finished, annealed |